MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Kraiburg TPE THERMOLAST® S TF4ZGOLCNT Thermoplastic Elastomer (FC/S Series)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: The FC/S series is a super-soft material solution for everyday life applications with regulatory requirements and outstanding dry and pleasant surface haptics. The compounds are available in translucent and can be colored in many different ways.

Processing Method: Injection Molding

Color / RAL DESIGN:

  • Translucent
Typical applications:
  • Cushioning
  • Protectors
  • Toys
  • Baits
  • Function and design elements
  • Fun articles
  • Seals
  • Bumpers
  • Grommets
Material advantages:
  • Soft, velvety feel
  • Dry haptics
  • Optimized mechanical properties at low hardnesses
  • Resilience
  • Elasticity
  • Precoloration in all colors
  • Colorable, also in effect colors
  • Free from animal ingredients
  • No silicones added
  • Suitable for processing in granule-based 3D printing

Information provided by Kraiburg TPE

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.873 g/cc0.0315 lb/in³DIN EN ISO 1183-1
Storage Temperature 15.0 - 30.0 °C59.0 - 86.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore OO 4545ASTM D 2240
Elongation at Break >= 1000 %>= 1000 %200 mm/min; DIN 53504/ISO 37
100% Modulus 0.100 MPa
@Strain 100 %
14.5 psi
@Strain 100 %
DIN 53504/ISO 37
300% Modulus 0.200 MPa
@Strain 300 %
29.0 psi
@Strain 300 %
DIN 53504/ISO 37
 
Descriptive Properties
ColorTranslucent
VLRH Hardness60DIN ISO 48-3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKRAIA8432 / 309096

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.