MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC NORYL™ Resin 731F Polyphenylene Ether + PS (PPE+PS) (Americas)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Unreinforced

Material Notes: NORYL™ 731F resin is a non-reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This NSF/ANSI 61* listed for potable water use, FDA Food Contact compliant, injection moldable grade exhibits good surface appearance, high ductility, and good impact resistance along with low moisture absorption, creep resistance, dimensional stability, and hydrolytic stability. NORYL 731F resin is an excellent candidate for a variety of water management applications such as valves, filtration components, and water meter internals.

Features: Hydrolytic Stability,Low Creep Sensitivity

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.06 g/ccASTM D792
Density 1.06 g/ccISO 1183
Water Absorption 0.060 %
@Time 86400 sec
ASTM D570
Moisture Absorption 0.0200 %Injection Molding
 0.0600 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.23 %ISO 62-1
Viscosity 9.0 cP
@Load 5.00 kg,
Temperature 280 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
SABIC method
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 9.2 g/10 min
@Load 5.00 kg,
Temperature 280 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 119ASTM D785
Tensile Strength at Break 49.0 MPa50 mm/min; ASTM D638
 51.0 MPa50 mm/min; ISO 527
Tensile Strength, Yield 57.0 MPa50 mm/min; ISO 527
 58.0 MPa50 mm/min; ASTM D638
Elongation at Break 17 %50 mm/min; ISO 527
 28.1 %50 mm/min; ASTM D638
Elongation at Yield 3.5 %50 mm/min; ISO 527
 7.2 %50 mm/min; ASTM D638
Tensile Modulus 2700 MPa1 mm/min; ISO 527
 2860 MPa50 mm/min; ASTM D638
Flexural Strength 89.0 MPayld, 2.6 mm/min, 100 mm span; ASTM D790
 90.0 MPayld, 1.3 mm/min, 50 mm span; ASTM D790
 95.0 MPayield, 2 mm/min; ISO 178
Flexural Modulus 2420 MPa2.6 mm/min, 100 mm span; ASTM D790
 2550 MPa2 mm/min; ISO 178
 2640 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 213 JASTM D256
 133 J
@Temperature -40.0 °C
ASTM D256
Izod Impact, Notched (ISO) 17.0 kJ/m²80*10*4; ISO 180/1A
 5.00 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Charpy Impact, Notched 17.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
Gardner Impact 5.00 J
@Temperature -40.0 °C
ASTM D3029
 25.0 J
@Temperature -30.0 °C
ASTM D3029
Dart Drop, Total Energy 48.0 JASTM D3763
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 2.65
@Frequency 50.0 - 60.0 Hz
ASTM D150
Dielectric Strength 21.6 kV/mm
@Thickness 3.20 mm
in oil; ASTM D149
Dissipation Factor 0.00040
@Frequency 50.0 - 60.0 Hz
ASTM D150
Arc Resistance 0.00 - 60 secASTM D495
Comparative Tracking Index 175 - 250 VUL 746A
Hot Wire Ignition, HWI 7.0 - 15 sec
@Thickness >=6.00 mm
UL 746A
 30 - 60 sec
@Thickness >=1.50 mm
UL 746A
High Amp Arc Ignition, HAI 0.00 - 15 arcs
@Thickness >=6.00 mm
UL 746A
 >= 120 arcs
@Thickness >=1.50 mm
UL 746A
High Voltage Arc-Tracking Rate, HVTR >= 150 mm/minUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 91.8 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 91.8 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 95.4 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 95.4 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 131 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 137 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 120 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 117 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 126 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Vicat Softening Point 140 °CRate B/50; ISO 306
 143 °CRate B/120; ISO 306
 148 °CRate B/50; ASTM D1525
UL RTI, Electrical 105 °CUL 746B
UL RTI, Mechanical with Impact 90.0 °CUL 746B
UL RTI, Mechanical without Impact 105 °CUL 746B
Flammability, UL94 HB
@Thickness >=1.50 mm
UL 94
Oxygen Index 22 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 280 - 310 °C
Zone 2 260 - 305 °C
Zone 3 270 - 310 °C
Melt Temperature 280 - 310 °CInjection Molding
Mold Temperature 75.0 - 105 °C
Drying Temperature 105 - 110 °CInjection Molding
Dry Time 3.00 - 4.00 hourInjection Molding
 8.00 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa
Shot Size 30 - 70 %
Screw Speed 20 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82251 / 290198

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.