System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Celanese Hytrel® HTR8745 BK320 TPC-ET
Categories:
Polymer
;
Thermoplastic
;
Elastomer, TPE
;
Polyester TPE
Material Notes:
45 Shore D, Heat Stabilized, Black, High Performance High Flow Polyester Elastomer with Excellent Fatigue Resistance Developed for Blow Molding
Former DuPont product acquired by Celanese in 2022.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.14
g/cc
0.0412
lb/in³
ISO 1183
Linear Mold Shrinkage, Transverse
0.018
cm/cm
0.018
in/in
ISO 294-4, 2577
Melt Flow
6.5
g/10 min
@Load 10.0 kg,
Temperature 230 °C
6.5
g/10 min
@Load 22.0 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties
Metric
English
Comments
Hardness, Shore D
40
40
15s; ISO 48-4
<= 45
<= 45
ISO 48-4
Tensile Stress at Strain
4.00
MPa
@Strain 5.0 %
580
psi
@Strain 5.0 %
1BA specimen at 50mm/min; ISO 527-1/-2
6.80
MPa
@Strain 10 %
986
psi
@Strain 10 %
ISO 527-1/-2
13.0
MPa
@Strain 50 %
1890
psi
@Strain 50 %
ISO 527-1/-2
18.0
MPa
@Strain 100 %
2610
psi
@Strain 100 %
ISO 527-1/-2
Tear Strength
120
kN/m
685
pli
normal; ISO 34-1
120
kN/m
685
pli
parallel; ISO 34-1
Thermal Properties
Metric
English
Comments
Melting Point
203
°C
397
°F
10°C/min; ISO 11357-1/-3
Glass Transition Temp, Tg
-45.0
°C
-49.0
°F
10°C/min; ISO 11357-1/-2
Flame Spread
<=
80.0
mm/min
@Thickness 1.00 mm
<=
3.15
in/min
@Thickness 0.0394 in
ISO 3795 (FMVSS 302)
Processing Properties
Metric
English
Comments
Melt Temperature
240
°C
464
°F
Optimum, Injection
240
°C
464
°F
Optimum, Extrusion
230
-
250
°C
446
-
482
°F
Range, Injection
Mold Temperature
45.0
°C
113
°F
Optimum, Injection
45.0
-
55.0
°C
113
-
131
°F
Injection
Drying Temperature
110
°C
230
°F
Injection
Dry Time
2.00
-
4.00
hour
2.00
-
4.00
hour
Injection, Dehumidified Dryer
Moisture Content
<= 0.060 %
<= 0.060 %
Extrusion
<= 0.080 %
<= 0.080 %
Injection
Descriptive Properties
Drying Recommended
yes
Injection
FMVSS Class
B
ISO 3795 (FMVSS 302)
Part Marking Code
>TPC-ET<
ISO 11469
Polymer
TPC
Resin Identification
TPC-ET
ISO 1043
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PDSX5218m / 249174
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.