MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC LNP™ THERMOCOMP™ Compound PCAF04FRHH Polycarbonate + ABS (PC+ABS)
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Glass Fiber Filled

Material Notes: LNP THERMOCOMP PCA04FRHH compound is based on Polycarbonate/Acrylonitrile Butadiene Styrene (PC/ABS) blend containing 20 % glass fiber. Added features of this grade include: Non-Brominated, Non-Chlorinated Flame Retardants.

Features: High Stiffness,Flame Retardant,Non-Chlorinated,Non-Brominated,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.32 g/ccISO 1183
Moisture Absorption 0.0200 %Injection Molding
Viscosity 8.0 cP
@Load 5.00 kg,
Temperature 260 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cmSABIC method
Linear Mold Shrinkage, Transverse 0.0030 - 0.0050 cm/cmSABIC method
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 85.0 MPa5 mm/min; ISO 527
Tensile Modulus 6200 MPa1 mm/min; ISO 527
Flexural Strength 130 MPabreak, 2mm/min; ISO 178
Flexural Modulus 5800 MPa2 mm/min; ISO 178
Flexural Strain at Break 2.5 %2 mm/min; ISO 178
Izod Impact, Notched (ISO) 23.0 kJ/m²80*10*4; ISO 180/1A
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 100 - 175 VUL 746A
 150 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 118 °CEdgew 120*10*4 sp=100mm; ISO 75/Ae
Vicat Softening Point 130 °CRate B/120; ISO 306
UL RTI, Electrical 80.0 °CUL 746B
UL RTI, Mechanical with Impact 80.0 °CUL 746B
UL RTI, Mechanical without Impact 80.0 °CUL 746B
Flammability, UL94 V-0
@Thickness >=1.50 mm
UL 94
Glow Wire Ignition Temperature 825 °C
@Thickness 1.50 mm
IEC 60695-2-13
 825 °C
@Thickness 2.00 mm
IEC 60695-2-13
Glow Wire Flammability Index 960 °C
@Thickness 1.50 mm
IEC 60695-2-12
 960 °C
@Thickness 2.00 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 220 - 260 °C
Zone 2 220 - 260 °C
Zone 3 230 - 270 °C
Melt Temperature 230 - 270 °CInjection Molding
Mold Temperature 50.0 - 70.0 °C
Drying Temperature 80.0 - 90.0 °CInjection Molding
Dry Time 2.00 - 4.00 hourInjection Molding
Precipitation Temperature 60.0 - 80.0 °CHopper Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH81766 / 289713

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.