Description: NF-614e is a flame retardant (FR) expandable polystyrene grade containing pentane as a blowing agent and a brominated polymeric flame retardant as an FR additive. The product is delivered in the form of spherical beads with a bulk density of about 0.6 g/cm3 and is available in 1050 kg octabins. Applications: The properties of NF-614e make it suitable for the production of flame retardant thick-walled shapemoulded products and heavy insulation board by block moulding in accordance with ISO EN 11925-2 class E and DIN4102 B1/B2 Information provided by BEWi Synbra |