MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Hexcel® HexPly® M77HF Epoxy System
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: HexPly® M77HF prepreg is a fiber-reinforced modified epoxy resin system specifically designed for bladder molding or sheet wrap tube applications. Unique chemistry provides fully cured parts in only three minutes at 300°F (149°C).

Features

  • Quick cure, three minutes at 300°F (149°C)
  • Available in wide variety of carbon or glass tapes and fabrics
  • High temperature stability for hot de-mold
  • Low viscosity, 10 poise at 230°F (110°C)
Applications
  • Golf Shafts
  • Bicycle Components
  • Hockey Sticks
  • Arrow Shafts
  • Fishing Rods
  • Prosthetics

Information provided by Hexcel Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.34 g/cc
Viscosity 1000 cP
@Temperature 105 °C
Heat up @10°C
 1000 cP
@Temperature 130 °C
Heat up @5°C
 1100 cP
@Temperature 105 °C
Heat up @5°C
 1500 cP
@Temperature 100 °C
Heat up @2°C
 4.00e+6 cP
@Temperature 150 °C
Heat up @10°C
 1.00e+7 cP
@Temperature 20.0 °C
Heat up @10°C
 1.00e+7 cP
@Temperature 20.0 °C
Heat up @2°C
 1.00e+7 cP
@Temperature 120 °C
Heat up @2°C
 1.00e+7 cP
@Temperature 20.0 °C
Heat up @5°C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 81.0 MPa
Elongation at Break 3.70 %
Tensile Modulus 3.45 GPa
Fracture Toughness 1.28 ksi-in½K1C
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 130 °CDMTA
 
Processing PropertiesOriginal ValueComments
Cure Time <= 3.00 min
@Temperature 149 °C
 <= 5.00 min
@Temperature 135 °C
 <= 30.0 min
@Temperature 107 °C
Gel Time 3.00 min
@Temperature 135 °C
 4.00 min
@Temperature 127 °C
 6.50 min
@Temperature 121 °C
Shelf Life 18.0 Month
@Temperature -18.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHEXCB9154 / 322310

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.