MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Advanced Petrochem PP 1101P Propylene Homopolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Description: Advanced-PP 1101P is a propylene homopolymer fibre grade characterized by medium flowability, medium molecular weight distribution and medium crystallinity providing excellent and consistent process and product behavior. Advanced-PP 1101P is particularly suitable for the production of staple fibre, bulked continuous filaments (BCF), continuous filaments (CF). The product is comprised of an advanced pheno free stabilizer package providing superior gasfading resistance and inherent basic UV-stability.

Application: BCF / CF of higher dtex and relatively lower line speed than standard BCF grades.

Regulatory Information: The Grade Advanced-PP 1101P and additives incorporated comply with United States FDA Regulation 21CFR 177.1520 Olefin Polymers and European Regulation (EU) 10/2011 (and its amendments). Specific information is available upon request.

Information provided by Advanced Petrochemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.910 g/ccISO 1183
Melt Flow 18 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 70.0 MPaH 358/30; ISO 2039-1
Tensile Strength, Yield 35.0 MPa50 mm/min; ISO 527-2
Elongation at Break >= 50 %50 mm/min; ISO 527-2
Elongation at Yield 10 %50 mm/min; ISO 527-2
Modulus of Elasticity 1.50 GPa1 mm/min; ISO 527-2
Charpy Impact Unnotched 120 kJ/m²ISO 179/1eU
Charpy Impact, Notched 2.50 kJ/m²ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 163 °CISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °CISO 75-2
Vicat Softening Point 154 °C
@Load 1.02 kg
A50; ISO 306
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAVPC002 / 249450

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.