MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Copper Alloy, UNS C15715, H04 Temper, Wire
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: Hard

Fabrication Properties: Excellent Suitability – Soldering, Capacity for Being Cold Worked; Good Suitability – Brazing; Fair Suitability – Butt Weld; Poor Suitability – Spot Weld, Seam Weld, Capacity for Being Hot Formed

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.83 g/cc0.319 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength  496 MPa
@Thickness 2.54 mm
72000 psi
@Thickness 0.100 in
 524 MPa
@Thickness 1.27 mm
76000 psi
@Thickness 0.0500 in
 600 MPa
@Thickness 0.508 mm
87000 psi
@Thickness 0.0200 in
 607 MPa
@Thickness 0.356 mm
88000 psi
@Thickness 0.0140 in
Tensile Strength, Yield  469 MPa
@Thickness 2.54 mm
68000 psi
@Thickness 0.100 in
0.2% Offset
 496 MPa
@Thickness 1.27 mm
72000 psi
@Thickness 0.0500 in
0.2% Offset
 572 MPa
@Thickness 0.508 mm
83000 psi
@Thickness 0.0200 in
0.2% Offset
 579 MPa
@Thickness 0.356 mm
84000 psi
@Thickness 0.0140 in
0.2% Offset
Elongation at Break  1.0 %
@Thickness 0.356 mm
1.0 %
@Thickness 0.0140 in
 2.0 %
@Thickness 0.508 mm
2.0 %
@Thickness 0.0200 in
 2.0 %
@Thickness 2.54 mm
2.0 %
@Thickness 0.100 in
 2.0 %
@Thickness 1.27 mm
2.0 %
@Thickness 0.0500 in
Tensile Modulus 117 GPa17000 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000181 ohm-cm0.00000181 ohm-cm95% IACS
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.6 µm/m-°C
@Temperature 20.0 - 300 °C
9.20 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.377 J/g-°C0.0900 BTU/lb-°F
Thermal Conductivity 30.4 W/m-K211 BTU-in/hr-ft²-°F
Melting Point 1083 °C1981 °F
 
Descriptive Properties
Cold Work (%)99.20.1 in
 99.80.05 in
 99.90.014 in
 99.90.02 in
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC15715x8 / 291576

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.