Vydyne A 1515 GFB BK EST KW2 is standard flow, organic heat stabilized, 15% glass-beads and 15% glass-fiber reinforced PA66 resin. Available in black, this product is also lubricated for improved machine feed and flow. Glass-beads provide the molded parts with good surface finish and low warpage, while glass-fiber increase stiffness and strength.Information provided by Ascend Performance Materials. |