MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC EXTEM™ Resin XH1015 Thermoplastic Polyimide (TPI) (Europe)
Categories: Polymer; Thermoplastic; Polyimide, Thermoplastic

Material Notes: Thermoplastic Polyimide Extem* XH1015 Resin. Also UL rating 94V0 at 1.5 and 3.0.

Features: High Stiffness,Lead free reflow soldering capable,IR Transparent,Low Creep Sensitivity,High Strength,High Heat Resistance,Good dimensional stability,Flame Retardant,Thin Wall,High Flow

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.31 g/ccASTM D792
Density 1.31 g/ccISO 1183
Water Absorption 0.60 %
@Time 173000 sec
ASTM D570
Moisture Absorption 0.0200 %Injection Molding
Water Absorption at Saturation 2.3 %ISO 62-1
Linear Mold Shrinkage, Flow 0.010 - 0.012 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 10 g/10 min
@Load 6.60 kg,
Temperature 367 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 74.0 MPa5 mm/min; ISO 527
 96.0 MPa5 mm/min; ASTM D638
Tensile Strength, Yield 101 MPa5 mm/min; ISO 527
 103 MPa5 mm/min; ASTM D638
Elongation at Break 7.0 %5 mm/min; ISO 527
 10 %5 mm/min; ASTM D638
Elongation at Yield 6.0 %5 mm/min; ISO 527
 7.0 %5 mm/min; ASTM D638
Tensile Modulus 3100 MPa1 mm/min; ISO 527
 3420 MPa5 mm/min; ASTM D638
Flexural Strength 120 MPayield, 2 mm/min; ISO 178
 168 MPayld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2870 MPa2 mm/min; ISO 178
 3130 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 43.0 JASTM D256
Izod Impact, Notched (ISO) 4.00 kJ/m²80*10*4; ISO 180/1A
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 3.4
@Frequency 1e+6 Hz
ASTM D150
 3.5
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 25.0 kV/mm
@Thickness 1.60 mm
in air; ASTM D149
Comparative Tracking Index 125 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 50.0 µm/m-°C
@Temperature 23.0 - 150 °C
ISO 11359-2
CTE, linear, Transverse to Flow 51.0 µm/m-°C
@Temperature 23.0 - 150 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 250 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 223 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 235 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 237 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Vicat Softening Point 247 °CRate B/120; ISO 306
 250 °CRate B/50; ISO 306
 260 °CRate B/50; ASTM D1525
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 375 - 405 °C
Zone 2 370 - 400 °C
Zone 3 380 - 410 °C
Melt Temperature 380 - 410 °CInjection Molding
Mold Temperature 160 - 200 °C
Drying Temperature 175 °CInjection Molding
Dry Time 4.00 - 6.00 hourInjection Molding
 24.0 hourCumulative; Injection Molding
Back Pressure 5.00 - 10.0 MPa
Shot Size 40 - 70 %
Vent Depth 0.00250 - 0.00760 cm
 
Descriptive Properties
Intake (throat) temperature70-100 °C
Screw speed (Circumferential speed)<0.2 m/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH80058 / 288005

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.