MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC LNP™ THERMOCOMP™ Compound OF008E Polyphenylene Sulfide, Linear (PPS, Linear) (Asia)
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS)

Material Notes: LNP THERMOCOMP OF008E compound is based on linear Polyphenylene Sulfide (PPS) resin containing 40% glass fiber. Added features of this grade include: Easy Molding.

Features: High Stiffness,Easy Molding,Structural

Information provided by SABIC

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.68 g/cc0.0607 lb/in³ASTM D792
Linear Mold Shrinkage, Flow 0.0020 cm/cm0.0020 in/in24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.0080 cm/cm0.0080 in/in24hrs; ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 160 MPa23200 psiISO 527
 178 MPa25800 psiASTM D638
Elongation at Break 1.2 %1.2 %ISO 527
 1.7 %1.7 %ASTM D638
Flexural Strength 190 MPa27600 psiISO 178
 248 MPa36000 psiASTM D790
Flexural Modulus 13.4 GPa1940 ksiISO 178
 14.26 GPa2068 ksiASTM D790
Izod Impact Notched 101 J74.5 ft-lbASTM D256
Izod Impact, Unnotched 5.87 J/cm11.0 ft-lb/inASTM D4812
Izod Impact, Notched (ISO) 6.00 kJ/m²2.86 ft-lb/in²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 21.0 kJ/m²9.99 ft-lb/in²80*10*4; ISO 180/1U
Coefficient of Friction, Dynamic 0.660.66ASTM D3702 Modified: Manual
Coefficient of Friction, Static 0.870.87ASTM D3702 Modified: Manual
K (wear) Factor 483 x 10-8 mm³/N-M240 x 10-10 in³-min/ft-lb-hrWasher; ASTM D3702 Modified: Manual
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 26.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
14.4 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 268 °C514 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 261 °C
@Thickness 3.20 mm
502 °F
@Thickness 0.126 in
unannealed; ASTM D648
Flammability, UL94 V-0
@Thickness 0.450 mm
V-0
@Thickness 0.0177 in
UL 94 by SABIC-IP

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH81759 / 289706

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.