MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Master Bond MasterSil 151S Two part, silver filled, low outgassing silicone for bonding, sealing and coating
Categories: Polymer; Thermoset; Silicone

Material Notes: Master Bond MasterSil 151S is a two component, silver filled silicone with superb electrical conductivity along with good heat transfer properties. Part A has a smooth, paste consistency, Part B is a low viscosity liquid. The mix ratio is 100 to 5 by weight. Upon mixing, MasterSil 151S retains its smooth, paste consistency. The working life for a 50 gram mass is 6 to 12 hours. The best cure schedule options are 4-6 hours at 150 to 180°F and 2-3 hours at 190 to 210°F. The system has low shrinkage upon curing and reasonably good dimensional stability. MasterSil 151S bonds well to a wide variety of substrates including metals, ceramics, glass, composites as well as many types of rubber and plastics. The system has very good flexibility and elongation. Consequently, it can withstand aggressive thermal cycling as well as mechanical and thermal shocks. Its paste consistency allows it to be easily applied as an adhesive, sealant or coating. It can also be utilized as a form-in-place conductive gasketing material. Since it is an addition cured system it cures readily in thicknesses up to and beyond 1/4 inch thick. The color of Part A is silver and Part B is clear. The service temperature range is -80°F to +400°F. MasterSil 151S is most likely to be considered in aerospace, electronic, opto-electronic and specialty OEM applications, where excellent electrical conductivity, resounding flexibility, high temperature resistance and low outgassing, are necessary requirements.

Product Advantages:

  • After mixing, paste consistency
  • Exceptionally long working life
  • Cures well in deep and wide sections
  • Very good electrical conductivity
  • Vacuum compatible
Key Features:
  • Excellent electrical conductivity
  • Addition cured type system
  • Highly flexible & temperature resistant
  • NASA low outgassing

Information provided by Master Bond.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.00 g/cc1.00 g/ccPart B
 3.81 g/cc3.81 g/ccPart A
Viscosity 50 - 150 cP50 - 150 cPPart B
Linear Mold Shrinkage <= 0.0010 cm/cm<= 0.0010 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 80 - 9080 - 90
Tensile Strength 2.76 - 4.83 MPa400 - 700 psi
Elongation at Break 100 - 150 %100 - 150 %
Tensile Modulus <= 0.0207 GPa<= 3.00 ksi
Adhesive Bond Strength 0.689 - 2.07 MPa100 - 300 psiTensile lap shear, Al to Al
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 0.0040 ohm-cm>= 0.0040 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 150 - 200 µm/m-°C83.3 - 111 µin/in-°F
Thermal Conductivity 1.30 - 1.59 W/m-K9.00 - 11.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 204 °C399 °F
Minimum Service Temperature, Air -62.0 °C-79.6 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  120 - 180 min
@Temperature 87.8 - 98.9 °C
2.00 - 3.00 hour
@Temperature 190 - 210 °F
Option 2
 240 - 360 min
@Temperature 65.6 - 82.2 °C
4.00 - 6.00 hour
@Temperature 150 - 180 °F
Option 1
Working Life 360 - 720 min360 - 720 minWorking Life; 50 gram batch
Shelf Life 3.00 - 6.00 Month3.00 - 6.00 Month
 
Descriptive Properties
Mixing ratio100:5
ViscosityPart A: Smooth Paste

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMASTM643 / 268831

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.