MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Nouryon Perkadox 33 Dibenzoyl peroxide, 33% powder with inert fillers
Categories: Other Engineering Material

Material Notes: Perkadox 33 is a special low-concentration BPO formulation (33% peroxide) for curing mine bolts and chemical anchors. The low concentration allows for transporting the product as non-ADR grade. The formulation ensures easy mixing and handling.

CAS number: 94-36-0

EINECS/ELINCS No.: 202-327-6

Applications: For some special applications it is desirable to use a dry benzoyl peroxide powder as a catalyst. For these cases the benzoyl peroxide formulation Perkadox 33 was introduced, which is a mixture of benzoyl peroxide and filler. Perkadox 33 can be handled very easily and without risk. It contains no plasticizer and is lower concentrated than the usual benzoyl peroxide formulations, which makes dosing easier. One of the most important applications for Perkadox 33 is as a catalyst for putties based on unsaturated polyester resins. A putty containing an accelerated polyester resin and Perkadox 33 cures rapidly so that after a short time the surface can be sanded and polished. The putty is made of two components, viz.: a) A powder consisting of a mixture of filler with pigment and Perkadox 33 as a catalyst. b) A liquid component consisting of polyester resin and N,N-Dimethylaniline (10% formulation in aliphatic ester) or N,N-dimethylparatoluidine (10% formulation in aliphatic ester), or alternatively, a polyester resin with a built-in amine accelerator. When the putty has to be applied component a) and b) are mixed. The manufacturer of these putties should take care that the powder contains Perkadox 33 and the liquid component the Accelerator, in such amounts that after mixing the two components there is enough time to apply the putty.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.895 g/cc
Storage Temperature <= 25.0 °C
 
Thermal PropertiesOriginal ValueComments
Decomposition Temperature 60.0 °CSelf-Accelerating Decomposition Temperature
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Descriptive Properties
AppearanceWhite powder
Assay32.0-33.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PNOURY773 / 286296

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.