MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC LNP™ LUBRILOY™ Compound D20001 Polycarbonate (PC) (Europe)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LNP LUBRILOY D20001 compound is based on Polycarbonate (PC) resin containing proprietary lubricant. Added features of this grade include: Non-Brominated, Non-Chlorinated Flame Retardant, Wear Resistant.

Features: Flame Retardant,Wear resistant,Non-Chlorinated,Non-Brominated

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ASTM D792
 1.20 g/cc0.0434 lb/in³ISO 1183
Moisture Absorption 0.0200 %0.0200 %Injection Molding
 0.120 %0.120 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0050 cm/cm0.0050 in/in24hrs; ASTM D955
 0.0053 cm/cm0.0053 in/in24hrs; ISO 294
Linear Mold Shrinkage, Transverse 0.0057 cm/cm0.0057 in/in24hrs; ISO 294
 0.0060 cm/cm0.0060 in/in24hrs; ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 54.0 MPa7830 psiISO 527
 60.0 MPa8700 psiASTM D638
Tensile Strength, Yield 62.0 MPa8990 psiISO 527
 67.0 MPa9720 psiASTM D638
Elongation at Break 6.5 %6.5 %ASTM D638
 6.7 %6.7 %ISO 527
Elongation at Yield 4.3 %4.3 %ISO 527
 4.5 %4.5 %ASTM D638
Tensile Modulus 2.55 GPa370 ksi50 mm/min; ASTM D638
 2.60 GPa377 ksi1 mm/min; ISO 527
Flexural Strength 102 MPa14800 psiISO 178
 103 MPa14900 psiASTM D790
Flexural Modulus 2.80 GPa406 ksiISO 178
 2.82 GPa409 ksiASTM D790
Izod Impact Notched 141 J104 ft-lbASTM D256
Izod Impact, Unnotched 16.12 J/cm30.20 ft-lb/inASTM D4812
Izod Impact, Notched (ISO) 6.00 kJ/m²2.86 ft-lb/in²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 104 kJ/m²49.5 ft-lb/in²80*10*4; ISO 180/1U
Dart Drop, Total Energy 51.0 J37.6 ft-lbpeak; ASTM D3763
Coefficient of Friction, Dynamic 0.0900.090ASTM D3702 Modified: Manual
Coefficient of Friction, Static 0.220.22ASTM D3702 Modified: Manual
K (wear) Factor 60.4 x 10-8 mm³/N-M30.0 x 10-10 in³-min/ft-lb-hrWasher; ASTM D3702 Modified: Manual
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  65.7 µm/m-°C
@Temperature -40.0 - 40.0 °C
36.5 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 65.7 µm/m-°C
@Temperature -40.0 - 40.0 °C
36.5 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow  66.5 µm/m-°C
@Temperature -40.0 - 40.0 °C
36.9 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
 66.6 µm/m-°C
@Temperature -40.0 - 40.0 °C
37.0 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 97.0 °C
@Thickness 3.20 mm
207 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 94.0 °C201 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 89.0 °C
@Thickness 3.20 mm
192 °F
@Thickness 0.126 in
unannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Zone 2 255 - 265 °C491 - 509 °F
Zone 3 260 - 270 °C500 - 518 °F
Melt Temperature 255 - 290 °C491 - 554 °FInjection Molding
Mold Temperature 40.0 - 65.0 °C104 - 149 °F
Drying Temperature 80.0 °C176 °FInjection Molding
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa29.0 - 43.5 psi
Screw Speed 30 - 60 rpm30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH81129 / 289076

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.