MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Arkema Kepstan® 6002 PL PEKK
Categories: Polymer; Thermoplastic; Polyketone; PEKK, Unreinforced

Material Notes:

Information provided by Arkema Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.27 g/cc1.27 g/ccCoating; ISO 1183
Density 1.27 g/cc0.0459 lb/in³ISO 1183
Water Absorption <= 0.60 %
@Time 86400 sec
<= 0.60 %
@Time 24.0 hour
ISO 62-1
Thickness 50.0 - 75.0 microns1.97 - 2.95 milRecommended Coating Thickness
 
Mechanical PropertiesMetricEnglishComments
Taber Abrasion, mg/1000 Cycles 8.0 - 128.0 - 12Wheel CS 17, load 1 kg; ISO 9352
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 1020 ohm1020 ohmASTM D257
Surface Resistivity per Square 1020 ohm1020 ohmASTM D257
Dielectric Strength 84.0 kV/mm2130 kV/inDry; IEC 60243-1
 84.0 kV/mm2130 kV/inIEC 60243-1
 
Thermal PropertiesMetricEnglishComments
Melting Point 300 - 305 °C572 - 581 °FISO 1218
Flammability, UL94 V-0V-0on coated panel
Oxygen Index 38 %38 %Dry; ISO 4589-1/-2
 
Descriptive Properties
ColorNatural
Form as DeliveredPowder
Moisture SensitiveNo
Pencil Hardness5HECCA T4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PARKF651 / 291149

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.