MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Akrochem PROAID® AC 8XL Wax
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product Description: PROAID AC 8XL is a highly concentrated, non-staining, non-discoloring processing and dispersing aid compatible with most polymers (including fluoroelastomers). HNBR flow and release properties are especially aided by AC 8XL. PROAID AC 8XL improves mold flow and extrusion characteristics as well as improving dispersion of fillers and chemicals. Mold and mill release are vastly improved with finished parts smooth and glossy. Mold buildup is greatly reduced and Proaid AC 8XL does not effect adhesion, bonding, or physical properties when used in recommended amounts. Will not interfere with peroxide cures.

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.13 g/cc
 
Thermal PropertiesOriginal ValueComments
Softening Point 84.0 °C
 
Descriptive Properties
Appearancetan powder
Content<5%Free Fatty Acid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAKZCH351 / 315269

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.