MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
BASF Ultramid® B3WG13 BK00102 Nylon 6, 63% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 60% Glass Fiber Filled

Material Notes: Ultramid B3WG13 BK00102 is a 63% glass reinforced, injection molding, high modulus nylon designed to have high strength and stiffness for metal replacement applications. It also has excellent moldability and outstanding surface appearance.

Applications: Potential applications are mirror brackets, fuel lids, gas-assisted steering wheel inserts, ski bindings and bike rack clamps.

Information provided by BASF.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.74 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 155 MPaConditioned; ISO 527
 235 MPaDry; ISO 527
Elongation at Break 2.0 %Dry; ISO 527
Tensile Modulus 13400 MPaConditioned; ISO 527
 22000 MPaDry; ISO 527
Flexural Strength 355 MPaDry; ISO 178
Flexural Modulus 19000 MPaDry; ISO 178
Izod Impact, Notched (ISO) 15.0 kJ/m²Dry; ISO 180
Charpy Impact Unnotched 90.0 kJ/m²
@Temperature -30.0 °C
Dry; ISO 179
 90.0 kJ/m²
@Temperature 23.0 °C
Dry; ISO 179
Charpy Impact, Notched 13.0 kJ/m²
@Temperature -30.0 °C
Dry; ISO 179
 15.0 kJ/m²
@Temperature 23.0 °C
Dry; ISO 179
 
Thermal PropertiesOriginal ValueComments
Melting Point 220 °CISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 214 °CISO 75
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 275 - 300 °C
Middle Barrel Temperature 285 - 310 °C
Front Barrel Temperature 300 - 320 °C
Nozzle Temperature 300 - 320 °C
Melt Temperature 300 - 320 °C
Mold Temperature 80.0 - 95.0 °C
Drying Temperature 80.0 °C
@Time 7200 - 14400 sec
Moisture Content <= 0.12 %
Injection Pressure 500 - 1500 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBASF8966 / 254924

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.