MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
SABIC ULTEM™ Resin 2110EPR Polyetherimide (PEI) (Asia)
Categories: Polymer; Thermoplastic; Polyetherimide (PEI)

Material Notes: 10% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing.

Features: High Stiffness,Hydrolytic Stability,Chemical Resistance,Enhanced Electroplatability,Easy Flow,Low Smoke and Toxicity,Good Mechanicals in Broad Temperature Range,Low Creep Sensitivity,Low Shrinkage,Good metal adhesion,Amorphous,High Strength,General Purpose,High Heat Resistance,Good dimensional stability,Flame Retardant,Good Mold Release

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.35 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0070 - 0.0090 cm/cm
@Thickness 3.20 mm
SABIC method
Linear Mold Shrinkage, Transverse 0.0060 - 0.0080 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 19 g/10 min
@Load 6.60 kg,
Temperature 337 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 119 MPa5 mm/min; ASTM D638
Tensile Strength, Yield 119 MPa5 mm/min; ASTM D638
Elongation at Break 3.0 %5 mm/min; ASTM D638
Elongation at Yield 3.0 %5 mm/min; ASTM D638
Tensile Modulus 5240 MPa5 mm/min; ASTM D638
Flexural Strength 193 MPabrk, 2.6 mm/min, 100 mm span; ASTM D790
 199 MPayld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 4800 MPa1.3 mm/min, 50 mm span; ASTM D790
 5170 MPa2.6 mm/min, 100 mm span; ASTM D790
Izod Impact Notched 69.0 JASTM D256
 350 J
@Thickness 3.20 mm
reverse notched; ASTM D256
Izod Impact, Unnotched 534 J/mASTM D4812
Dart Drop, Total Energy 10.0 JASTM D3763
 
Electrical PropertiesOriginal ValueComments
Arc Resistance 60 - 120 secASTM D495
Comparative Tracking Index 100 - 175 VUL 746A
Hot Wire Ignition, HWI 7.0 - 15 sec
@Thickness >=0.400 mm
UL 746A
 30 - 60 sec
@Thickness >=0.750 mm
UL 746A
 60 - 120 sec
@Thickness >=3.00 mm
UL 746A
High Amp Arc Ignition, HAI 15 - 30 arcs
@Thickness >=0.400 mm
UL 746A
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/minUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 36.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
CTE, linear, Transverse to Flow 81.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 210 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 212 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 205 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 207 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Vicat Softening Point 210 °CRate B/50; ASTM D1525
UL RTI, Electrical 155 °CUL 746B
UL RTI, Mechanical with Impact 155 °CUL 746B
UL RTI, Mechanical without Impact 155 °CUL 746B
Flammability, UL94 V-0
@Thickness >=0.400 mm
UL 94

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82596 / 290543

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.