Cycoloy* RCX7233 (experimental grade name EXCY0355) resin is an injection moldable impact modified PC blend with non-brominated and non-chlorinated flame retardant. It contains 30% post consumer recycle content with a UL-94 V0 rating @ 0.75 mm for all color. Developed for applications require excellent flow and impact balance with thin wall flame resistance. Limited availability and restricted color only. Features: Flame Retardant,Non-Chlorinated,Non-Brominated Information provided by SABIC |