MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Stratasys® ABSplus FDM 3D Printing Polymer
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; ABS Polymer

Material Notes: ABSplus is an affordable FDM thermoplastic with production-grade durability offering a wide range of colors for concept modeling and rapid prototyping. ABSplus is a widely used FDM printing material that features high durability and fine details. Consisting of production-grade thermoplastics, parts 3D printed with ABSplus are affordable, mechanically strong and stable over time.

Characteristics

  • Opaque
  • Strong and durable
  • Impact resistant
  • Dimensionally stable
Options
  • Nine colors, plus the option for custom colors
  • Can be smoothed to achieve the gloss of injection-molded ABS
Uses
  • General-purpose prototyping
  • Concept models
  • Functional prototypes
  • Jigs and fixtures
  • Production parts
Advantages
  • Accurate, reliable functional testing with familiar ABS plastic
  • Hands-free support removal

Information provided by Proto3000

Key Words: Fused Deposition Modeling
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 109.5109.5ASTM D785
Tensile Strength, Ultimate 33.0 MPa
@Thickness 3.17 mm
4790 psi
@Thickness 0.125 in
Type 1, XZ Axis, 0.2?/min; ASTM D638
Tensile Strength, Yield 31.0 MPa
@Thickness 3.17 mm
4500 psi
@Thickness 0.125 in
Type 1, XZ Axis, 0.2?/min; ASTM D638
Elongation at Break 6.00 %
@Thickness 3.17 mm
6.00 %
@Thickness 0.125 in
Type 1, XZ Axis, 0.2?/min; ASTM D638
Elongation at Yield 2.00 %
@Thickness 3.17 mm
2.00 %
@Thickness 0.125 in
Type 1, XZ Axis, 0.2?/min; ASTM D638
Tensile Modulus 2.20 GPa
@Thickness 3.17 mm
319 ksi
@Thickness 0.125 in
Type 1, XZ Axis, 0.2?/min; ASTM D638
Flexural Strength 35.0 MPa5080 psiMethod 1, 0.05?/min, ZX Axis; ASTM D790
 58.0 MPa8410 psiMethod 1, 0.05?/min, XZ Axis; ASTM D790
Flexural Modulus 1.65 GPa239 ksiMethod 1, 0.05?/min, ZX Axis; ASTM D790
 2.10 GPa305 ksiMethod 1, 0.05?/min, XZ Axis; ASTM D790
Flexural Strain at Break 2.00 %2.00 %Method 1, 0.05?/min, XZ Axis; ASTM D790
 2.00 %2.00 %Method 1, 0.05?/min, ZX Axis; ASTM D790
Izod Impact, Notched 1.06 J/cm1.99 ft-lb/inMethod A, XZ Axis; ASTM D256
 
Thermal PropertiesMetricEnglishComments
CTE, linear 88.2 µm/m-°C49.0 µin/in-°FASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 96.0 °C205 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 82.0 °C180 °FASTM D648
Glass Transition Temp, Tg 108 °C226 °F
Flammability, UL94 HB
@Thickness 2.50 mm
HB
@Thickness 0.0984 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPROTO815 / 322828

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.