MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
HB Fuller 20RC Adhesive and Sealant
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: 20RC and 20RCHH are anaerobic resins that are the best method for retaining, locking, and sealing a wide range of metal parts. Even in the tightest fitting assemblies voids are presents which allows for movement and potential loosening of the parts. 20RC and 20RCHH form a tough, durable resin, that fills all these voids, creating a unitized assembly that is completely resistant to shock, vibration, and extremely harsh environmental conditions. These materials cure in the absence of air and in the present of metal. They are ideally suited for retaining cylindrical assemblies providing shock and vibration resistance.

Features and Benefits:

  • Green Anaerobic Retaining Compound and Sealant
  • High Strength
  • Excellent Gap and Void Filling Capability
  • High Resistance to Heat, Corrosion, Vibrations, Water, Gases, Oils, Hydrocarbons, and Many Chemicals

Information provided by H.B. Fuller Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/cc
Brookfield Viscosity 8000 cP20RC, Spindle 5, 20 rpm
 12000 cP20RCHV, Spindle 5, 20 rpm
Storage Temperature 8.00 - 28.0 °C
 
Mechanical PropertiesOriginal ValueComments
Shear Strength >= 13.8 MPaPin/Collar
 
Thermal PropertiesOriginal ValueComments
CTE, linear 80.0 µm/m-°CASTM D696
Specific Heat Capacity 0.300 J/g-°C
Thermal Conductivity 0.100 W/m-KASTM C177
Maximum Service Temperature, Air 150 °C
Minimum Service Temperature, Air -55.0 °C
Flash Point >= 100 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 12.0 - 72.0 hourSet Time on Steel, Full Cure
Shelf Life 12.0 Month
 
Descriptive Properties
ColorGreen
ConsistencyViscous Liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHBFULL207 / 316998

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.