MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Akrochem VERSAMAG™ Magnesium hydroxide
Categories: Other Engineering Material

Material Notes: Product Description: Versamag (magnesium hydroxide) is an inert filler, flame retardant smoke suppressant for latex foam, elastomeric goods, epoxies, reinforced polyesters, phenolics, and urethane foam. Magnesium hydroxide releases its 31% water of crystallization when heated to above 325°C as water vapor. The high temperature of water release allows for processing of engineered plastics without moisture entering into the molding operation. The resulting endothermic reaction cools the product below flash point, reducing the risk of fire. The vapor released also helps reduce smoke, an additional advantage of this type flame retardant. Char formation is also improved over alumina trihydrate. Magnesium hydroxide also functions as an excellent acid acceptor in a chlorinated polyethylene (CPE) non-peroxide, thiadiazole cure system providing better scorch time as well as faster cure than magnesium oxide. Mg(OH)2 has also been shown to prevent premature scorch vs. MgO in Hypalon formulas.

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.36 g/cc
Bulk Density 0.200 - 0.300 g/cc
Particle Size 2.0 µm
Particle Mesh Size 325 Mesh0.2% Residue
Specific Surface Area 18 m²/g
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 1.0 %
@Temperature 110 °C
 
Component Elements PropertiesOriginal ValueComments
CaO 1.2 %
Loss on Ignition(%) >= 30.5 %
 
Descriptive Properties
Appearancewhite powder
Assay0.96Dried
Content0.004Soluble Salts

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAKZCH285 / 315203

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.