MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

Mitsubishi PLA-X³ 3D Printing Filament
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Renewable/Recycled Polymer; Thermoplastic; Polylactic Acid (PLA) Biopolymer

Material Notes: PLA-X3 is a industrial high-performance PLA which features extreme performance on speed, mechanical properties and high heat environments. PLA-X3 is perfect for printing speeds of >120 mm/s, increasing efficiency. Users who use a lot of ABS now have a bio-based alternative material with all the advantages of ABS and none of the disadvantages like shrinking and delamination. PLA-X3 has been specifically engineered for industrial applications for an easy to print filament with high mechanical properties. Objects that are printed with PLA-X3 will have a semi matte finish which not only looks great but helps concealing layer lines.

Features:

  • Prints like PLA, performs like ABS
  • Engineered for fast printing (>120mm/s)
  • ABS matching mechanical properties
  • Great heat resistance at higher temperatures
  • HDT after annealing 95°C+
  • Semi matte finish after printing
  • Negligible shrinkage after annealing
Colors: PLA is available from stock in 6 colors.

Information provided by Mitsubishi Chemical.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.27 g/cc1.27 g/ccISO 1183
Filament Diameter 1750 µm1750 µmTolerance: 50 µm, =95% Roundness
 2850 µm2850 µmTolerance: 100 µm, =95% Roundness
Melt Flow 6.0 g/10 min
@Load 2.16 kg,
Temperature 210 °C
6.0 g/10 min
@Load 4.76 lb,
Temperature 410 °F
ISO 1133
Storage Temperature 15.0 - 25.0 °C59.0 - 77.0 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 40.0 MPa5800 psiISO 527
Elongation at Break 47 %47 %ISO 527
Tensile Modulus 4.00 GPa580 ksi(E); ISO 527
Charpy Impact, Notched 2.30 J/cm²10.9 ft-lb/in²ISO 179
 
Thermal PropertiesMetricEnglishComments
Melting Point 190 - 220 °C374 - 428 °F
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C203 °FISO 75
 
Processing PropertiesMetricEnglishComments
Processing Temperature 220 - 240 °C428 - 464 °FPrinting Temperature, based on speed
 
Descriptive Properties
Bed Temp±50-60°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMITS9840 / 301065

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.