Veradel® A-101 is a very low melt flow general purpose amorphous PESU resin for extrusion and injection molding. This transparent grade offers high heat deflection temperature, excellent toughness and dimensional stability and resistance to mineral acids. Other desirable properties include thermal stability, creep resistance and inherent flame resistance. This grade was formerly marketed as Radel® A PESU. - Natural: Veradel® A-101 NT Applications: Film; Sheet; Tubing Features: Acid Resistant; Creep Resistant; Flame Retardant; Food Contact Acceptable; Good Dimensional Stability; Good Thermal Stability; Good Toughness; Steam Resistant Information provided by Solvay Specialty Polymers. |