MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC CYCOLOY™ CP8320 PC+ABS (Asia)
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced

Material Notes: CYCOLOY Medium Heat Plating Grade for Automotive

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 g/cc1.10 g/ccASTM D792
Density 1.10 g/cc0.0397 lb/in³ISO 1183
Water Absorption 0.30 %0.30 %23°C/sat; ISO 62
Moisture Absorption 0.100 %0.100 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
0.0050 - 0.0070 in/in
@Thickness 0.126 in
SABIC method
Melt Flow  13 g/10 min
@Load 5.00 kg,
Temperature 260 °C
13 g/10 min
@Load 11.0 lb,
Temperature 500 °F
cm³/10 min; ISO 1133
 14 g/10 min
@Load 5.00 kg,
Temperature 260 °C
14 g/10 min
@Load 11.0 lb,
Temperature 500 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 40.0 MPa5800 psi50 mm/min; ASTM D638
 40.0 MPa5800 psi50 mm/min; ISO 527
Tensile Strength, Yield 45.0 MPa6530 psi50 mm/min; ISO 527
 45.0 MPa6530 psi50 mm/min; ASTM D638
Elongation at Break 100 %100 %50 mm/min; ISO 527
 100 %100 %50 mm/min; ASTM D638
Elongation at Yield 4.0 %4.0 %50 mm/min; ISO 527
 4.0 %4.0 %50 mm/min; ASTM D638
Tensile Modulus 2.10 GPa305 ksi1mm/min; ISO 527
 2.10 GPa305 ksi5 mm/min; ASTM D638
Flexural Yield Strength 65.0 MPa9430 psi2 mm/min; ISO 178
 70.0 MPa10200 psi1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.00 GPa290 ksi1.3 mm/min, 50 mm span; ASTM D790
 2.00 GPa290 ksi2 mm/min; ISO 178
Izod Impact, Notched 6.00 J/cm11.2 ft-lb/inASTM D256
 4.00 J/cm
@Temperature -30.0 °C
7.49 ft-lb/in
@Temperature -22.0 °F
ASTM D256
Izod Impact, Notched (ISO) 60.0 kJ/m²28.6 ft-lb/in²80*10*3; ISO 180/1A
 30.0 kJ/m²
@Temperature -30.0 °C
14.3 ft-lb/in²
@Temperature -22.0 °F
80*10*3; ISO 180/1A
Charpy Impact, Notched 6.00 J/cm²28.6 ft-lb/in²Edgew 80*10*3 sp=62mm; ISO 179/1eA
 3.00 J/cm²
@Temperature -30.0 °C
14.3 ft-lb/in²
@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 55.0 J40.6 ft-lbASTM D3763
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohm>= 1.00e+15 ohmROA; IEC 60093
Dielectric Strength  17.0 kV/mm
@Thickness 3.20 mm
432 kV/in
@Thickness 0.126 in
in oil; IEC 60243-1
 25.0 kV/mm
@Thickness 1.60 mm
635 kV/in
@Thickness 0.0630 in
in oil; IEC 60243-1
 35.0 kV/mm
@Thickness 0.800 mm
889 kV/in
@Thickness 0.0315 in
in oil; IEC 60243-1
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  90.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
50.0 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 90.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
50.0 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow  90.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
50.0 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 90.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
50.0 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
Thermal Conductivity 0.200 W/m-K1.39 BTU-in/hr-ft²-°FISO 8302
Hot Ball Pressure Test 75.0 °C167 °FIEC 60695-10-2
Deflection Temperature at 1.8 MPa (264 psi) 92.0 °C198 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 90.0 °C
@Thickness 3.20 mm
194 °F
@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 106 °C223 °FRate B/50; ISO 306
 106 °C223 °FRate B/50; ASTM D1525
 107 °C225 °FRate B/120; ISO 306
 
Processing PropertiesMetricEnglishComments
Processing Temperature 60.0 - 80.0 °C140 - 176 °FHopper Temperature
Nozzle Temperature 230 - 270 °C446 - 518 °FInjection Molding
Zone 1 220 - 250 °C428 - 482 °F
Zone 2 240 - 280 °C464 - 536 °F
Zone 3 240 - 280 °C464 - 536 °F
Melt Temperature 250 - 280 °C482 - 536 °F
Mold Temperature 60.0 - 90.0 °C140 - 194 °F
Drying Temperature 95.0 - 105 °C203 - 221 °FInjection Molding
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourInjection Molding
Moisture Content 0.020 %0.020 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABI10747 / 244214

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.