NORYL™ PPO534 resin is a non-reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This high heat injection moldable grade exhibits high impact strength, dimensional stability, hydrolytic stability, and very low moisture absorption. This material is an excellent candidate for compounding applications. Information provided by SABIC |