MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC LNP™ STAT-KON™ Compound DX04490R Polycarbonate (PC)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LNP STAT-KON DX04490R compound is based on Polycarbonate (PC) resin containing proprietary fillers. Added features of this grade include: Electrically Conductive, Radar Absorbing.

Features: Radar Absorption,Electrically Conductive

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.23 g/cc0.0444 lb/in³ASTM D792
 1.23 g/cc0.0444 lb/in³ISO 1183
Moisture Absorption 0.0200 %0.0200 %Injection Molding
 0.200 %0.200 %23°C/50% RH/24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0040 cm/cm0.0040 in/in24hrs; ASTM D955
 0.0042 cm/cm0.0042 in/in24hrs; ISO 294
Linear Mold Shrinkage, Transverse 0.0050 cm/cm0.0050 in/in24hrs; ASTM D955
 0.0050 cm/cm0.0050 in/in24hrs; ISO 294
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 60.0 MPa8700 psiASTM D638
 61.0 MPa8850 psiISO 527
Elongation at Break 8.5 %8.5 %ISO 527
 16.3 %16.3 %ASTM D638
Elongation at Yield 4.2 %4.2 %ASTM D638
 4.5 %4.5 %ISO 527
Tensile Modulus 2.71 GPa393 ksi1 mm/min; ISO 527
 2.98 GPa432 ksi50 mm/min; ASTM D638
Flexural Strength 75.0 MPa10900 psiISO 178
 89.0 MPa12900 psiASTM D790
Flexural Modulus 2.51 GPa364 ksiISO 178
 2.71 GPa393 ksiASTM D790
Izod Impact Notched 48.0 J35.4 ft-lbASTM D256
Izod Impact, Unnotched 23.42 J/cm43.88 ft-lb/inASTM D4812
Izod Impact, Notched (ISO) 5.00 kJ/m²2.38 ft-lb/in²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 167 kJ/m²79.5 ft-lb/in²80*10*4; ISO 180/1U
Dart Drop, Total Energy 4.00 J2.95 ft-lbpeak; ASTM D3763
Impact Test 9.00 J6.64 ft-lbMultiaxial Impact; ISO 6603
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 100 ohm-cm - 1e+05100 ohm-cm - 1e+05ASTM D257
Surface Resistance 100 ohm - 1e+05100 ohm - 1e+05ASTM D257
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  63.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
35.0 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 63.5 µm/m-°C
@Temperature -40.0 - 40.0 °C
35.3 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow  59.4 µm/m-°C
@Temperature -40.0 - 40.0 °C
33.0 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 60.8 µm/m-°C
@Temperature -40.0 - 40.0 °C
33.8 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 133 °C271 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 132 °C
@Thickness 3.20 mm
270 °F
@Thickness 0.126 in
unannealed; ASTM D648
UL RTI, Electrical 80.0 °C176 °FUL 746B
UL RTI, Mechanical with Impact 80.0 °C176 °FUL 746B
UL RTI, Mechanical without Impact 80.0 °C176 °FUL 746B
Flammability, UL94 HB
@Thickness >=1.50 mm
HB
@Thickness >=0.0591 in
UL 94
 
Processing PropertiesMetricEnglishComments
Zone 2 310 - 320 °C590 - 608 °F
Zone 3 320 - 330 °C608 - 626 °F
Melt Temperature 305 - 325 °C581 - 617 °FInjection Molding
Mold Temperature 80.0 - 110 °C176 - 230 °F
Drying Temperature 120 °C248 °FInjection Molding
Dry Time 4.00 hour4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa29.0 - 43.5 psi
Screw Speed 30 - 60 rpm30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH81252 / 289199

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.