MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC LNP™ LUBRICOMP™ Compound WBL36L Polybutylene Terephthalate (PBT) (Asia)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Unreinforced, Molded

Material Notes: LNP LUBRICOMP WBL36L compound is based on Polybutylene Terephthalate (PBT) resin containing 30% glass bead, 15% PTFE. Added features of this grade include: Wear Resistant, Low Extractables.

Features: Low Extractable,Good dimensional stability,Wear resistant,Low Warpage,Food Contact Acceptable

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.69 g/cc0.0611 lb/in³ASTM D792
 1.69 g/cc0.0611 lb/in³ISO 1183
Moisture Absorption 0.0400 %0.0400 %23°C/50% RH/24 hrs; ASTM D570
 0.0500 %0.0500 %Injection Molding
Linear Mold Shrinkage, Flow 0.010 - 0.030 cm/cm0.010 - 0.030 in/in24hrs; ASTM D955
 0.024 cm/cm0.024 in/in24hrs; ISO 294
 0.024 cm/cm0.024 in/inSABIC method
Linear Mold Shrinkage, Transverse 0.017 - 0.020 cm/cm0.017 - 0.020 in/in24hrs; ASTM D955
 0.019 cm/cm0.019 in/in24hrs; ISO 294
 0.019 cm/cm0.019 in/inSABIC method
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 36.0 MPa5220 psi5 mm/min; ASTM D638
 36.0 MPa5220 psi5 mm/min; ISO 527
Tensile Strength, Yield 37.0 MPa5370 psi5 mm/min; ASTM D638
 37.0 MPa5370 psi5 mm/min; ISO 527
Elongation at Break 3.1 %3.1 %5 mm/min; ASTM D638
 3.4 %3.4 %5 mm/min; ISO 527
Elongation at Yield 2.2 %2.2 %5 mm/min; ASTM D638
 2.4 %2.4 %5 mm/min; ISO 527
Tensile Modulus 4.02 GPa583 ksi1 mm/min; ISO 527
 4.13 GPa599 ksi50 mm/min; ASTM D638
Flexural Strength 74.0 MPa10700 psiyld, 1.3 mm/min, 50 mm span; ASTM D790
 75.0 MPa10900 psiyield, 2 mm/min; ISO 178
Flexural Modulus 3.90 GPa566 ksi1.3 mm/min, 50 mm span; ASTM D790
 4.14 GPa600 ksi2 mm/min; ISO 178
Izod Impact Notched 32.0 J23.6 ft-lbASTM D256
Izod Impact, Unnotched 2.56 J/cm4.80 ft-lb/inASTM D4812
Izod Impact, Notched (ISO) 3.00 kJ/m²1.43 ft-lb/in²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 18.0 kJ/m²8.57 ft-lb/in²80*10*4; ISO 180/1U
Dart Drop, Total Energy 3.00 J2.21 ft-lbpeak; ASTM D3763
Impact Test 1.00 J0.738 ft-lbMultiaxial Impact; ISO 6603
Coefficient of Friction, Dynamic 0.660.66ASTM D3702 Modified: Manual
Coefficient of Friction, Static 0.630.63ASTM D3702 Modified: Manual
K (wear) Factor 50.4 x 10-8 mm³/N-M25.0 x 10-10 in³-min/ft-lb-hrWasher; ASTM D3702 Modified: Manual
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  73.8 µm/m-°C
@Temperature -40.0 - 40.0 °C
41.0 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 74.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
41.1 µin/in-°F
@Temperature 73.4 - 140 °F
ISO 11359-2
 74.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
41.1 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow  70.2 µm/m-°C
@Temperature -40.0 - 40.0 °C
39.0 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 71.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
39.4 µin/in-°F
@Temperature 73.4 - 140 °F
ISO 11359-2
 71.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
39.4 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 184 °C363 °FFlatw 80*10*4 sp=64mm; ISO 75/Bf
 188 °C
@Thickness 3.20 mm
370 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 94.0 °C201 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 95.0 °C
@Thickness 3.20 mm
203 °F
@Thickness 0.126 in
unannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Zone 2 240 - 250 °C464 - 482 °F
Zone 3 250 - 260 °C482 - 500 °F
Melt Temperature 240 - 250 °C464 - 482 °FInjection Molding
Mold Temperature 80.0 - 100 °C176 - 212 °F
Drying Temperature 120 °C248 °FInjection Molding
Dry Time 4.00 hour4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa29.0 - 43.5 psi
Screw Speed 30 - 60 rpm30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH81078 / 289025

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.