MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC NORYL™ Resin HMC3008V Polyphenylene Ether + PS (PPE+PS)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Unreinforced

Material Notes: NORYL HMC3008V compound is based on Polyphenylene Ether (PPE) resin containing carbon fiber, glass fiber and minerals (total 26%). Added features of this grade include: Electrically Conductive, Non-Halogenated Flame Retardant, Dimensional Stability.

Features: Good dimensional stability,Flame Retardant,Non-Halogenated,Electrically Conductive

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.259 g/cc1.259 g/ccASTM D792
Melt Flow 10.6 g/10 min
@Load 5.00 kg,
Temperature 300 °C
10.6 g/10 min
@Load 11.0 lb,
Temperature 572 °F
ASTM D1238
Ash 17.82 %17.82 %
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 120.67 MPa17502 psi10 mm/min; SABIC - Japan Method
Elongation at Break 6.6 %6.6 %10 mm/min; SABIC - Japan Method
Flexural Strength 155 MPa22500 psiyld, 2.6 mm/min, 100 mm span; ASTM D790
Flexural Modulus 9.719 GPa1410 ksi2.6 mm/min, 100 mm span; ASTM D790
Izod Impact Notched 66.4 J49.0 ft-lbASTM D256
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 42000 ohm42000 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 133.4 °C
@Thickness 6.40 mm
272.1 °F
@Thickness 0.252 in
unannealed; ASTM D648
Flammability, UL94  V-1
@Thickness >=1.50 mm
V-1
@Thickness >=0.0591 in
UL 94
 V-0
@Thickness >=3.00 mm
V-0
@Thickness >=0.118 in
UL 94
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 290 - 310 °C554 - 590 °F
Zone 2 270 - 290 °C518 - 554 °F
Zone 3 280 - 300 °C536 - 572 °F
Melt Temperature 290 - 310 °C554 - 590 °FInjection Molding
Mold Temperature 80.0 - 110 °C176 - 230 °F
Drying Temperature 120 °C248 °FInjection Molding
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH82333 / 290280

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.