MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
SABIC LEXAN™ Copolymer SLX2471T Polycarbonate (PC) (Asia)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors

Features: Weatherable

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccASTM D792
Density 1.20 g/ccISO 1183
Moisture Absorption 0.0200 %Injection Molding
 0.150 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.35 %ISO 62-1
Viscosity 9.0 cP
@Load 1.20 kg,
Temperature 300 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 10 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 70.0 MPa50 mm/min; ISO 527
 73.0 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 65.0 MPa50 mm/min; ASTM D638
 65.0 MPa50 mm/min; ISO 527
Elongation at Break >= 100 %50 mm/min; ASTM D638
 >= 100 %50 mm/min; ISO 527
Elongation at Yield 6.0 %50 mm/min; ISO 527
 6.4 %50 mm/min; ASTM D638
Tensile Modulus 2300 MPa1 mm/min; ISO 527
 2400 MPa5 mm/min; ASTM D638
Flexural Strength 100 MPayld, 1.3 mm/min, 50 mm span; ASTM D790
 100 MPayield, 2 mm/min; ISO 178
Flexural Modulus 2450 MPa1.3 mm/min, 50 mm span; ASTM D790
 2450 MPa2 mm/min; ISO 178
Izod Impact Notched 820 JASTM D256
 130 J
@Temperature -30.0 °C
ASTM D256
Izod Impact, Notched (ISO) 65.0 kJ/m²80*10*3; ISO 180/1A
 10.0 kJ/m²
@Temperature -30.0 °C
80*10*3; ISO 180/1A
Izod Impact, Unnotched (ISO) NB80*10*3; ISO 180/1U
Charpy Impact Unnotched NBEdgew 80*10*3 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 65.0 kJ/m²Edgew 80*10*3 sp=62mm; ISO 179/1eA
 15.0 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*3 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 85.0 JASTM D3763
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 175 - 250 VUL 746A
Hot Wire Ignition, HWI 30 - 60 sec
@Thickness >=1.00 mm
UL 746A
 >= 120 sec
@Thickness >=3.00 mm
UL 746A
High Amp Arc Ignition, HAI 60 - 120 arcs
@Thickness >=1.00 mm
UL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 70.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 70.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 70.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 70.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Hot Ball Pressure Test 75.0 °CPASS; IEC 60695-10-2
 125 °CPASS; IEC 60695-10-2
Deflection Temperature at 1.8 MPa (264 psi) 125 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 126 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 140 °CRate B/50; ASTM D1525
 140 °CRate B/50; ISO 306
 141 °CRate B/120; ISO 306
UL RTI, Electrical 110 °CUL 746B
UL RTI, Mechanical with Impact 110 °CUL 746B
UL RTI, Mechanical without Impact 110 °CUL 746B
Flammability, UL94 V-2
@Thickness >=1.50 mm
UL 94
Glow Wire Ignition Temperature 850 °C
@Thickness 1.00 mm
IEC 60695-2-13
 850 °C
@Thickness 1.50 mm
IEC 60695-2-13
 850 °C
@Thickness 3.00 mm
IEC 60695-2-13
Glow Wire Flammability Index 900 °C
@Thickness 1.50 mm
IEC 60695-2-12
 960 °C
@Thickness 3.00 mm
IEC 60695-2-12
 960 °C
@Thickness 1.00 mm
IEC 60695-2-12
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.59ISO 489
Haze 0.20 %
@Thickness 2.54 mm
ASTM D1003
Transmission, Visible 89 %
@Thickness 2.54 mm
ASTM D1003
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 275 - 295 °C
Zone 2 265 - 290 °C
Zone 3 280 - 300 °C
Melt Temperature 280 - 300 °CInjection Molding
Mold Temperature 70.0 - 95.0 °C
Drying Temperature 120 °CInjection Molding
Dry Time 3.00 - 4.00 hourInjection Molding
 48.0 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa
Shot Size 40 - 60 %
Vent Depth 0.00250 - 0.00760 cm
Screw Speed 40 - 70 rpm
 
Descriptive Properties
UV-light, water exposure/immersionF1UL 746C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH80426 / 288373

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.