MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Aquivion® D79-25BS-Li Perfluorosulfonic Acid Lithium Salt (PFSA Lithium Salt)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Fluoropolymer

Material Notes: Aquivion® D79-25BS-Li is a chemically-stabilized (denoted by the S-suffix) perfluorosulfonic acid (PFSA) lithium salt dispersion that exhibits an Equivalent Weight (EW) of 790 g/eq. Polymer concentration is 25 percent. Solvent system is >99% water and is free of ethers.

Aquivion® PFSA lithium salt dispersion is based on the Short Side Chain copolymer of Tetrafluoroethylene (TFE) and Sulfonyl Fluoride Vinyl Ether (SFVE) F2C=CF-O-CF2CF2-SO2F produced by Solvay. The resulting perfluoropolymer's functional groups are in their lithium sulfonate form, (-SO3Li).

Once formulated with solvents, Aquivion® D79-25BS-Li can be used for the preparation of cast films or coatings on various substrates. Formulations with volatile and non-volatile additives can be used to make components for electrochemical devices.

HEALTH, SAFETY AND ENVIRONMENT
- Aquivion® D79-25BS-Li is not harmful if used and handled according to standard processing procedures (see for example the "Guide to the Safe Handling of Fluoropolymer Resins" issued by the Society of the Plastics Industry). If handled improperly(e.g. overheating above 260°C (500°F) for an extended period of time) the dispersion may release harmful toxic chemicals. Please refer to corresponding Material Safety Data Sheets (SDS) for more information on handling and safety.

PACKAGING, SHIPMENT AND STORAGE
- Aquivion® PFSA D79-25BS-Li is available in 5 and 60 liter containers. It is recommended to store the product at 25 °C (77 °F) in a clean temperature-controlled and well ventilated environment, protected from direct sunlight and other sources of heat or irradiation. Containers should be kept tightly closed to avoid solvent evaporation.

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.15 g/ccASTM D1475
 
Descriptive Properties
Availability (as of March 2019)Asia Pacific; Europe; North America

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y5090 / 238471

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.