MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Ganpati Exim Basic Chrome Sulphate 24-26% Chromium
Categories: Other Engineering Material

Material Notes: Basic Chrome Sulphate is the most important ingredient used in the tanning of leather. It is manufactured from the simple reduction of Cr (VI) to Cr (III) by the addition of an excess of sulphur dioxide: Na2Cr2O7 + 3SO2 + H2O ? Cr2(SO4)2(OH)2 + Na2SO4 This reaction is carried out in a steam-heated vessel, and then the excess SO2 is removed in a second reaction tower. Finally, the liquid product is spray-dried to form a powder which is then bagged and sold. As dichromate is a highly poisonous compound, all emissions from the plant are closely monitored and all sump water is recycled and the chromium within it reused.

Information provided by Ganpati Exim PVT. LTD.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Component Elements PropertiesOriginal ValueComments
Cr2O3 24 - 26 %
Iron, Fe <= 0.10 %
 
Descriptive Properties
Basicity>33%
Water insoluable<0.1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGANPATI099 / 317383

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.