MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

SABIC LNP™ ELCRES™ EXL9334 Polycarbonate (PC)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LNP ELCRES EXL9334 is based on Polycarbonate (PC) siloxane copolymer resin. It is a UV stabilized, medium flow opaque material suitable for injection molding (IM) and sheet extrusion applications. This grade offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, non-chlorine FR systems, extreme low temperature ductility (-40°C) characteristics and excellent processability with opportunities for shorter IM cycle times compared to standard PC. It is available in a wide range of opaque colors and may be an excellent candidate for a wide range of applications.

Features: Enhanced Low Temperature Impact,Flame Retardant,UV Resistant,Non-Chlorinated,Non-Brominated,High Impact Resistance,Exceptional Processing

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.19 g/cc1.19 g/ccASTM D792
Density 1.19 g/cc0.0430 lb/in³ISO 1183
Moisture Absorption 0.0200 %0.0200 %Injection Molding
 0.150 %0.150 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.40 %0.40 %ISO 62-1
Viscosity 9.0 cP
@Load 1.20 kg,
Temperature 300 °C
9.0 cP
@Load 2.65 lb,
Temperature 572 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0040 - 0.0080 cm/cm0.0040 - 0.0080 in/inSABIC method
Linear Mold Shrinkage, Transverse 0.0040 - 0.0080 cm/cm0.0040 - 0.0080 in/inSABIC method
Melt Flow 10 g/10 min
@Load 1.20 kg,
Temperature 300 °C
10 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 57.0 MPa8270 psi50 mm/min; ISO 527
 59.0 MPa8560 psi50 mm/min; ASTM D638
Tensile Strength, Yield 56.0 MPa8120 psi50 mm/min; ISO 527
 58.0 MPa8410 psi50 mm/min; ASTM D638
Elongation at Break 108 %108 %50 mm/min; ISO 527
 115 %115 %50 mm/min; ASTM D638
Elongation at Yield 6.0 %6.0 %50 mm/min; ASTM D638
 6.0 %6.0 %50 mm/min; ISO 527
Tensile Modulus 2.00 GPa290 ksi1 mm/min; ISO 527
 2.10 GPa305 ksi5 mm/min; ASTM D638
Flexural Strength 87.0 MPa12600 psiyield, 2 mm/min; ISO 178
 89.0 MPa12900 psiyld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.05 GPa297 ksi1.3 mm/min, 50 mm span; ASTM D790
 2.10 GPa305 ksi2 mm/min; ISO 178
Izod Impact Notched 750 J553 ft-lbASTM D256
 685 J
@Temperature -40.0 °C
505 ft-lb
@Temperature -40.0 °F
ASTM D256
 725 J
@Temperature -30.0 °C
535 ft-lb
@Temperature -22.0 °F
ASTM D256
Izod Impact, Unnotched NBNBASTM D4812
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ASTM D4812
Izod Impact, Notched (ISO) 65.0 kJ/m²30.9 ft-lb/in²80*10*3; ISO 180/1A
Izod Impact, Unnotched (ISO) NBNB80*10*3; ISO 180/1U
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
80*10*3; ISO 180/1U
Charpy Impact Unnotched NBNBEdgew 80*10*3 sp=62mm; ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 7.00 J/cm²33.3 ft-lb/in²Edgew 80*10*3 sp=62mm; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmASTM D257
Comparative Tracking Index 175 - 250 V175 - 250 VUL 746A
Hot Wire Ignition, HWI  15 - 30 sec
@Thickness 0.750 mm
15 - 30 sec
@Thickness 0.0295 in
UL 746A
 30 - 60 sec
@Thickness 3.00 mm
30 - 60 sec
@Thickness 0.118 in
UL 746A
High Amp Arc Ignition, HAI  60 - 120 arcs
@Thickness 0.750 mm
60 - 120 arcs
@Thickness 0.0295 in
UL 746A
 >= 120 arcs
@Thickness 3.00 mm
>= 120 arcs
@Thickness 0.118 in
UL 746A
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  61.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
33.9 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 61.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
33.9 µin/in-°F
@Temperature 73.4 - 176 °F
ISO 11359-2
CTE, linear, Transverse to Flow  62.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
34.4 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 65.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
36.1 µin/in-°F
@Temperature 73.4 - 176 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 140 °C
@Thickness 3.20 mm
284 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 118 °C244 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 123 °C
@Thickness 3.20 mm
253 °F
@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 139 °C282 °FRate B/50; ISO 306
 140 °C284 °FRate B/50; ASTM D1525
 141 °C286 °FRate B/120; ISO 306
UL RTI, Electrical 125 °C257 °FUL 746B
UL RTI, Mechanical with Impact 110 °C230 °FUL 746B
UL RTI, Mechanical without Impact 120 °C248 °FUL 746B
Flammability, UL94  V-0
@Thickness >=1.50 mm
V-0
@Thickness >=0.0591 in
UL 94
 5VA
@Thickness >=3.00 mm
5VA
@Thickness >=0.118 in
UL 94
Glow Wire Ignition Temperature 825 °C
@Thickness 1.50 mm
1520 °F
@Thickness 0.0591 in
IEC 60695-2-13
Glow Wire Flammability Index 960 °C
@Thickness 1.50 mm
1760 °F
@Thickness 0.0591 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 290 - 310 °C554 - 590 °F
Zone 2 280 - 305 °C536 - 581 °F
Zone 3 295 - 315 °C563 - 599 °F
Melt Temperature 295 - 315 °C563 - 599 °FInjection Molding
Mold Temperature 70.0 - 95.0 °C158 - 203 °F
Drying Temperature 120 °C248 °FInjection Molding
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hourInjection Molding
 48.0 hour48.0 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Shot Size 40 - 60 %40 - 60 %
Vent Depth 0.00250 - 0.00760 cm0.000984 - 0.00299 in
Screw Speed 40 - 70 rpm40 - 70 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH80594 / 288541

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.