MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Go Yen Chemical GY-FRB53 Flame Retardant
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: GY-FR-B53 is a brominated flame retardant that not only has excellent and effective flame-retardant effects for thermoplastic resin, but also offers good thermal stability and great UV stability which allows the end-product to be used under indoor fluorescent or temporary outdoor sunlight. It can be used in SAN, Polysulfone, ABS, PC, PC/ABS blends, PET, PBT, and PET/PBT blends. Due to its high purity, GY-FR-B53 can be used for applications that required good thermal and electrical properties.

Intro: Technology Department of GYC Group specializes in research and development, also devotes our efforts to satisfying customers’ needs. We are also the greatest supplier of flame retardants in Asia. GY-FR-B53 is a brominated flame retardant that not only has excellent and effective flame-retardant effects for thermoplastic resin, but also offers good thermal stability and great UV stability which allows the end-product to be used under indoor fluorescent or temporary outdoor sunlight. It can be used in SAN, Polysulfone, ABS, PC, PC/ABS blends, PET, PBT, and PET/PBT blends. Due to its high purity, GY-FR-B53 can be used for applications that required good thermal and electrical properties.

Advantages:

  • A high performance flame retardant with excellent flame retardant efficiency
  • Commonly used in thermoplastic resin
  • Provide great UV stability
  • Provide good thermal stability
  • Allow the end-product to be used under indoor fluorescent or temporary outdoor sunlight
  • Brominated flame retardant with a high purity
Applications:
  • Highly effective in thermoplastic resin applications
  • Commonly used in SAN and Polysulfone
  • Commonly used in ABS, PC, and PC/ABS blends
  • Commonly used in PET, PBT, and PET/PBT blends
  • Can be used for applications that required good thermal and electrical properties

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesOriginal ValueComments
Melting Point 200 - 230 °C
 
Component Elements PropertiesOriginal ValueComments
Bromine, Br 58.0 %
 
Descriptive Properties
AppearancePowder
ColorWhite
Whiteness>95

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGOYEN034 / 266342

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.