MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Syensqo (Solvay Specialty Polymers) Ixef® GS-1022 Polyarylamide (PARA), 50% glass fiber
Categories: Polymer; Thermoplastic; Polyarylamide (PAA); Polyarylamide, Glass Fiber Filled

Material Notes: 50% glass fiber, gamma stabilized for healthcare

Ixef® GS-1022 is a 50% glass-fiber reinforced grade of polyarylamide (PARA) available in several colors. Parts molded from these colored resins can withstand high-energy gamma radiation without significant change in appearance and physical properties. Ixef® GS-1022 resins demonstrate no evidence of cytotoxicity, sensitization, intracutaneous reactivity or acute systemic toxicity, based on biocompatibility testing as defined by ISO 10993-1.

This resin offers superior strength and stiffness combined with outstanding surface gloss and exceptional flow and is well suited for medical applications, such as single use surgical instruments and structural device housings, and applications in food service equipment.

Colors available:
- Brown: GS-1022 BN01
- Blue: GS-1022 BU01
- Green: GS-1022 GN01
- Grey: GS-1022 GY01
- Grey: GS-1022 GY02
- Grey: GS-1022 GY51
- White: GS-1022 WH01

Markets/Uses: Healthcare / Medical Devices / Dental Instruments; Healthcare / Medical Devices / Medical Parts/Thin Walls; Healthcare / Medical Devices / Medical Single Use Applications; Healthcare / Medical Devices / Medical/Healthcare Applications; Healthcare / Medical Devices / Orthopedics; Healthcare / Medical Devices / Sizing Trials; Healthcare / Medical Devices / Surgical Instruments

Applications: Dental Applications; Hospital Goods; Medical Devices; Medical/Healthcare Applications; Surgical Instruments

Features: Biocompatible; Chemical Resistant; Creep Resistant; E-beam Sterilizable; Ethylene Oxide Sterilizable; Good Dimensional Stability; Good Sterilizability; High Flow; High Strength; Low Moisture Absorption; Outstanding Surface Finish; Radiation (Gamma) Resistant; Radiation Sterilizable; Radiotranslucent; Ultra High Stiffness

Property values for individual batches will vary within specification limits. Values shown are typical of Ixef GS-1022/WH01 resin; other colorants may alter values.

There will be a shift in color when comparing pre-gamma sterilization and post-gamma sterilization colors. It is also expected that the colors will revert to some degree, back toward the as-molded color. Lighter colors may display the greatest variation.

Injection notes: Hot runners: 250° to 260°C (482° to 500°F)
Storage
Ixef® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Ixef® resins be dried prior to molding following the recommendations found in this datasheet and/or in the Ixef® processing guide.

Information provided by Solvay Specialty Polymers.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.78 g/cc0.0643 lb/in³ISO 1183
Water Absorption 0.28 %
@Time 86400 sec
0.28 %
@Time 24.0 hour
ISO 62
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cm0.0010 - 0.0030 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 265 MPa38400 psiISO 527-2
Elongation at Break 1.8 %1.8 %ISO 527-2
Tensile Modulus 22.0 GPa3190 ksiISO 527-2
Flexural Strength 380 MPa55100 psiISO 178
Flexural Modulus 22.0 GPa3190 ksiISO 178
Izod Impact, Unnotched (ISO) 50.0 kJ/m²23.8 ft-lb/in²ISO 180
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 15.0 µm/m-°C8.33 µin/in-°FISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 230 °C446 °FUnannealed; ISO 75-2/A
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 250 - 260 °C482 - 500 °F
Front Barrel Temperature 260 - 290 °C500 - 554 °F
Nozzle Temperature 260 - 290 °C500 - 554 °F
Melt Temperature 280 °C536 °FInjection
Mold Temperature 120 - 140 °C248 - 284 °F
Drying Temperature 120 °C
@Time 1800 - 5400 sec
248 °F
@Time 0.500 - 1.50 hour
 
Descriptive Properties
AdditiveGamma Stabilizer
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorColors Available
FormsPellets
Injection RateFast
ProcessingInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y4295 / 280095

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.