Ultramid Advanced N3HG6 is a partially aromatic, 30% glass fiber reinforced polyphthalamide for injection molding with strong mechanical properties especially at elevated temperatures, good longterm thermal stability and outstanding chemical resistance for highly stressed parts. This material has high toughness, stiffness, extremely low water absorption and outstanding dimensional stability. It features high flowability and allows filling of complex parts with thin wall thickness. It is easily processable with excellent melt stability.Information provided by BASF. |