MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Go Yen Chemical Goyenchem-144 High Effective Anti-Fish eyes & Volcanic Vents Agent
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Intro: GO YEN CHEMICAL INDUSTRIAL CO., LTD. (GYC Group) is the most innovative fine chemical fine chemical manufacturer in Taiwan. We own the strongest R&D team and abundant functional product line. We heard the voice from clients and solve the problems during manufacturing and R&D. GYC have developed Goyenchem-144 especially for coating, paint, ink industries to prevent and remove fish eyes and volcanic vents in paint, coating, ink application,Goyenchem-144 can enhance the adherence of topcoat and can release and eliminate the odor in coating. Besides, Goyenchem-144 imparts coating excellent smoothness and also enhances the adding value. Furthermore, Goyenchem-144 has adopted and earned the reputation from several domestic and abroad renowned factories.

Advantages:

  • Prevent fish eyes and volcanic vents on the top of coating
  • Sustain the smoothness of shaped products
  • Enhance the heat resistance of product during bake
  • To avoid poor performing caused by mix unevenly or bad dispersion
  • Enhance the adherence of topcoat
  • With excellent compatibility with various surface treatment, coating and resin

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.850 - 0.950 g/cc
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.375 - 1.425
 
Descriptive Properties
AppearanceClear

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGOYEN346 / 266654

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.