MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Go Yen Chemical GY-WMB50C Matting Agent Masterbatch
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: GY-WMB50C has excellent compatibility with polyolefin (PP, PE, HDPE, LDPE, EVA, EPDM, EPR), TPV, TPO, POE, etc. during the compound procedure. Unlike the conventional silica matting agents which are in light weight and are easy to produce dust during the processing, GY-WMB50C not only has high specific weight but also with the property of excellent heat tolerance. Additionally, since GY-WMB50C will not adhere the screws during the processing, injection molding and extrusion molding are both applicable.

Advantages:

  • Excellent matting effect
  • Reduce the gloss of a product and make it low glare
  • In the type of masterbatch which is easy to operate for the technicians and can be directly processed with plastics
  • Excellent ink absorbency which improves the tinting strength of plastic products during the printing process
  • Improve the printability of plastic products
  • Excellent processability
  • Excellent thermostability
  • Excellent dispersiblity
  • Will not adhere the screws during the processing
  • Applicable to injection molding and extrusion molding
Applications:
  • Polyolefin matting applications: PP, PE, HDPE, LDPE, EVA TPV , TPO, POE matting applications
  • General plastics or engineering plastics
  • Packaging materials, shopping bags, garbage bags, films…
  • Cables and wires
  • For injection molding and extrusion molding

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.90 g/cc
Melt Flow <= 1.0 g/10 min
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.20 %
 
Descriptive Properties
AppearancePellet
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGOYEN459 / 266767

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.