MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Polyram PB330I8 Nylon 6, 40% Mineral/Glass Filled Heat Stabilized
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Glass/Mineral Reinforced

Material Notes: Information provided by Polymer Technology and Services, LLC (PTS).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.38 g/ccDIN 53479
Linear Mold Shrinkage 0.0025 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 122ASTM D785
Tensile Strength, Yield 17400 psi
@Thickness 3.17 mm
ASTM D638
Elongation at Break 3.5 %
@Thickness 3.17 mm
ASTM D638
Flexural Strength 36260 psi
@Thickness 3.17 mm
ASTM D790
Flexural Modulus 1.09e+6 psi
@Thickness 3.17 mm
ASTM D790
Izod Impact, Notched 0.930 ft-lb/in
@Thickness 3.17 mm
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Melting Point 424 °FASTM D789
Maximum Service Temperature, Air 110 °CContinuous
Flammability, UL94 HB
@Thickness 3.00 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Clariant Renol 60G33HSL Nylon 6, 33% Glass Fiber Reinforced, Heat Stabilized, Lubricated
Clariant Renol PA133 Nylon 66, Highly Impact Modified, Heat Stabilized, Lubricated
Techmer ES HiFill® PA6 GF/M40 HS L BK 40% Glass/Mineral Filled

PPOLYRA425 / 57665

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.