MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Angst+Pfister APSOplast® PF CC 201 Laminated fabric, Hgw 2082
Categories: Polymer; Thermoset

Material Notes: (laminated fabric sheets made from phenolic resin and fine cotton fabric)

Thanks to the use of fine cotton fabric, this laminated fabric has very good mechani cal properties. This construction grade is particularly suitable for parts with high demands in mechanical engineering. If value is placed upon particularly good dielectric properties – ensuring that parts are suitable for purposes where good insulation is required – type PF CC 202 (Hgw 2082.5) is recommended. This material is manufactured using special resins and electrolyte-free fabric.

Information provided by Angst + Pfister

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.30 - 1.40 g/cc0.0470 - 0.0506 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 80.0 MPa11600 psiISO 527
Modulus of Elasticity 7.00 GPa1020 ksiflexural test; ISO 178
Flexural Strength 130 MPa18900 psiISO 178
Charpy Impact Unnotched 0.880 J/cm²4.19 ft-lb/in²ISO 179/3C
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 1.00e+6 ohm1.00e+6 ohmafter 24 h immersed in water; IEC 60167
Dielectric Constant 5.05.0DIN 53483
Dielectric Strength 2.00 kV/mm50.8 kV/inat 90°C in oil parallel to layers; IEC 60243-1
Comparative Tracking Index 100 V100 V[kV], at 90°C in oil parallel to layers; IEC 60243-1
 
Thermal PropertiesMetricEnglishComments
CTE, linear 20.0 - 40.0 µm/m-°C11.1 - 22.2 µin/in-°FVDE 0304/2
Thermal Conductivity 0.200 W/m-K1.39 BTU-in/hr-ft²-°FDIN 52612
 
Descriptive Properties
Colorbrown
Disruptive discharge voltage5
Water Absorption100[mg], 4 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PANGP098 / 250596

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.