MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Marco Polo MARPOL LL4M 899 Linear Low Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: MARPOL® LL4M 899 exhibits an excellent flow for high speed injection molding of lids, while providing good tear resistance and ESCR.

Recommended Applications: Injection molding – lids.

Additives: Slip – no, Antiblock - no.

Information provided by Marco Polo International, LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.929 g/cc0.0336 lb/in³ASTM D1505
Melt Flow 105 g/10 min
@Load 2.16 kg,
Temperature 190 °C
105 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5959ASTM D2240
Tensile Strength at Break 13.0 MPa1890 psiASTM D638
Tensile Strength, Yield 16.0 MPa2320 psiASTM D638
Elongation at Yield 9.3 %9.3 %ASTM D638
Flexural Modulus, 1% Secant 520 MPa75400 psiASTM D790
2% Secant Modulus 0.483 GPa70.0 ksiFlexure Secant; ASTM D790
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 86.0 °C187 °FASTM D1525
Brittleness Temperature -60.0 °C-76.0 °FF50; ASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMARCO155 / 283752

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.