MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI adhesives

(Viewing data as-entered. Click here to return)
SABIC CYCOLOY™ HC1204HF PC+ABS (Asia)
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced

Material Notes: High heat PC/ABS blend offering good flow and excellent impact. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI).

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.15 g/ccASTM D792
Density 1.15 g/ccISO 1183
Water Absorption 0.60 %23°C/sat; ISO 62
Moisture Absorption 0.200 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cmSABIC method
 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 8.0 g/10 min
@Load 2.16 kg,
Temperature 260 °C
cm³/10 min; ISO 1133
 22 g/10 min
@Load 5.00 kg,
Temperature 260 °C
cm³/10 min; ISO 1133
 24 g/10 min
@Load 5.00 kg,
Temperature 260 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 115ISO 2039-2
Ball Indentation Hardness 96.0 MPaISO 2039-1
Tensile Strength at Break 45.0 MPa50 mm/min; ISO 527
 45.0 MPa5 mm/min; ISO 527
 47.0 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 55.0 MPa5 mm/min; ISO 527
 55.0 MPa50 mm/min; ISO 527
 57.0 MPa50 mm/min; ASTM D638
Elongation at Break >= 50 %50mm/min; ISO 527
 100 %5 mm/min; ISO 527
 100 %50 mm/min; ASTM D638
Elongation at Yield 4.0 %50 mm/min; ISO 527
 5.0 %5 mm/min; ISO 527
 5.0 %50 mm/min; ASTM D638
Tensile Modulus 2270 MPa5 mm/min; ASTM D638
 2400 MPa1mm/min; ISO 527
Flexural Yield Strength 80.0 MPa2 mm/min; ISO 178
 88.0 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2300 MPa2 mm/min; ISO 178
 2300 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 580 J/mASTM D256
 480 J/m
@Temperature -30.0 °C
ASTM D256
Izod Impact, Notched (ISO) 50.0 kJ/m²80*10*3; ISO 180/1A
 30.0 kJ/m²
@Temperature -30.0 °C
80*10*3; ISO 180/1A
Charpy Impact, Notched 50.0 kJ/m²Edgew 80*10*3 sp=62mm; ISO 179/1eA
 30.0 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*3 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 54.0 JASTM D3763
Taber Abrasion, mg/1000 Cycles 63CS-17, 1 kg; SABIC method
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohmROA; IEC 60093
Dielectric Constant 2.7
@Frequency 1e+6 Hz
IEC 60250
 2.8
@Frequency 50.0 - 60.0 Hz
IEC 60250
Dielectric Strength 17.0 kV/mm
@Thickness 3.20 mm
in oil; IEC 60243-1
 25.0 kV/mm
@Thickness 1.60 mm
in oil; IEC 60243-1
 35.0 kV/mm
@Thickness 0.800 mm
in oil; IEC 60243-1
Dissipation Factor 0.0020
@Frequency 50.0 - 60.0 Hz
IEC 60250
 0.0070
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 250 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 72.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 80.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 72.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 80.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
ISO 11359-2
Thermal Conductivity 0.200 W/m-KISO 8302
Hot Ball Pressure Test 125 °CIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 122 °CEdgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi) 102 °C1.8 MPa Edgew 120*10*4 sp=100mm; ISO 75/Ae
 112 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 126 °CRate B/50; ISO 306
 128 °CRate B/120; ISO 306
 130 °CRate B/50; ASTM D1525
UL RTI, Electrical 105 °CUL 746B
UL RTI, Mechanical with Impact 80.0 °CUL 746B
UL RTI, Mechanical without Impact 105 °CUL 746B
Flammability, UL94 HB
@Thickness 3.00 mm
UL 94
 HB
@Thickness 1.20 mm
UL 94
Oxygen Index 23 %ISO 4589
Glow Wire Test 650 °C
@Thickness 1.00 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Processing Temperature 60.0 - 80.0 °CHopper Temperature
Nozzle Temperature 240 - 280 °CInjection Molding
Zone 1 230 - 260 °C
Zone 2 250 - 290 °C
Zone 3 250 - 290 °C
Melt Temperature 260 - 290 °C
Mold Temperature 60.0 - 90.0 °C
Drying Temperature 100 - 110 °CInjection Molding
Dry Time 2.00 - 4.00 hourInjection Molding
Moisture Content 0.020 %
 
Compliance PropertiesOriginal ValueComments
USP Class VI Yes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10752 / 244219

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.