Product Description: 30% Glass Fiber, Heat Stabilized, Bio-based polyamide 5.6 Resin ID (ISO 1043): PAGF30 Filler / Reinforcement: Glass Fiber, 30% Filler by Weight Additive: Heat Stabilized Processing: Injection Molding Color: Black Information provided by Petropol |