MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Alfa Chemistry Materials Lutetium Metal
Categories: Metal

Material Notes: Lutetium is a lustrous, soft, ductile, silvery-white metal. It occurs in minimal amounts in most minerals containing yttrium. The pure metal has only recently been isolated and is one of the most difficult to prepare. Lutetium is relatively stable in air and reacts slowly with water. Lutetium Metal, is the hardest metal of the rare-earths, used as important additive to some specialty alloy. Stable Lutetium can be used as catalysts in petroleum cracking in refineries and can also be used in alkylation, hydrogenation, and polymerization applications. Lutetium is used as a phosphor in LED light bulbs. Lutetium Metal can be further processed to various shapes of ingots, pieces, wires, foils, slabs, rods, discs and powder.

Applications: is the hardest metal of the rare-earths, used as important additive to some specialty alloy. Lutetium Metal can be further processed to various shapes of ingots, pieces, wires, foils, slabs, rods, discs and powder, please visit Rare Earth Metals & Sputtering Targets page for more detailed information.

Molecular Formula: Lu

Room temperature, dryAlfa Chemistry Materials product group: Metal

Manufacturer data sheet

Vendors: Alfa Chemistry is an ISO 9001:2015 certified supplier of various materials, including: MOFs, coatings, nanomaterials, metals, polymers, carbon fibers, graphite, ceramics, glass, semiconductors, catalysts, carbon nanotubes, fullerene, COFs, molecular sieve, quantum dots, recycled plastics, photonic and optical materials, and magnetic materials, for customers worldwide. Alfa Chemistry also provides custom synthesis services for nearly all kinds of materials and chemicals. Learn more about Alfa Chemistry's high quality products at materials.alfachemic.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 9.84 g/cc0.355 lb/in³
Molecular Weight 175 g/mol175 g/mol
 
Thermal PropertiesMetricEnglishComments
Melting Point 1652 °C3006 °F
Boiling Point 3402 °C6156 °F
 
Descriptive Properties
AppearanceSilvery
CAS Number7439-94-3
Purity99.999% 99.99% 99.9% 99%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

ZZALFA66582 / 304050

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.