MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP Technology PA12 SLS Black Nylon 12 for SLS 3D Printing
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: Good mechanical properties, low density, resistant to abrasion, water, and solvents.

Distinguished for its dark black color, PA12 SLS Black is a versatile cost-effective ally for a wide range of industrial applications in many sectors:- connectors, hinges, housings and enclosures, jigs and fixtures just to cite a few. By PA12 SLS Black allows complex geometries and thin walls even for small objects, including functional prototypes, small series, and limited editions.

Information provided by CRP Technology.

Key Words: Selective Laser Sintering
Vendors:   About CRP Technology
CRP Technology (Modena, Italy) develops, manufactures and sells its proprietary high performance composite materials Windform® for professional 3D Printing. It is also distinguished by its know-how in Selective Laser Sintering technology. It offers part production for short- and low-run production, and prototyping services with Windform®. Its specific application fields including but are not limited to: automotive and motorsports, design, aerospace, UAVs, marine, entertainment, defense, and packaging.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 0.990 g/cc0.0358 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7878UNI EN ISO 868
Tensile Strength at Break 45.78 MPa6640 psiZX Axis; UNI EN ISO 527-1
 47.84 MPa6939 psiXY Axis; UNI EN ISO 527-1
 47.92 MPa6950 psiYX Axis; UNI EN ISO 527-1
Elongation at Break 8.7 %8.7 %ZX Axis; UNI EN ISO 527-1
 11.06 %11.06 %YX Axis; UNI EN ISO 527-1
 12.18 %12.18 %XY Axis; UNI EN ISO 527-1
Tensile Modulus 1.868 GPa270.9 ksiZX Axis; UNI EN ISO 527-1
 1.907 GPa276.6 ksiXY Axis; UNI EN ISO 527-1
 1.919 GPa278.3 ksiYX Axis; UNI EN ISO 527-1
Flexural Strength 68.84 MPa9984 psiUNI EN ISO 14125
Flexural Modulus 1.628 GPa236.1 ksiUNI EN ISO 14125
Izod Impact, Notched (ISO)  4.70 kJ/m²
@Temperature -40.0 °C
2.24 ft-lb/in²
@Temperature -40.0 °F
UNI EN ISO 180
 4.90 kJ/m²
@Temperature 23.0 °C
2.33 ft-lb/in²
@Temperature 73.4 °F
UNI EN ISO 180
Izod Impact, Unnotched (ISO)  18.5 kJ/m²
@Temperature -40.0 °C
8.80 ft-lb/in²
@Temperature -40.0 °F
UNI EN ISO 180
 19.9 kJ/m²
@Temperature 23.0 °C
9.47 ft-lb/in²
@Temperature 73.4 °F
UNI EN ISO 180
Charpy Impact Unnotched  2.26 J/cm²
@Temperature -30.0 °C
10.8 ft-lb/in²
@Temperature -22.0 °F
UNI EN ISO 179-1
 2.54 J/cm²
@Temperature 23.0 °C
12.1 ft-lb/in²
@Temperature 73.4 °F
UNI EN ISO 179-1
Charpy Impact, Notched  0.400 J/cm²
@Temperature -30.0 °C
1.90 ft-lb/in²
@Temperature -22.0 °F
UNI EN ISO 179-1
 0.430 J/cm²
@Temperature 23.0 °C
2.05 ft-lb/in²
@Temperature 73.4 °F
UNI EN ISO 179-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.5e+14 ohm-cm1.5e+14 ohm-cmASTM D257-14
Surface Resistance 9.3e+14 ohm9.3e+14 ohmASTM D257-14
Comparative Tracking Index 600 V600 VIEC 60112 Solution A
 
Thermal PropertiesMetricEnglishComments
Melting Point 181.7 °C359.1 °FISO 11357
 
Descriptive Properties
ColorDark Black
Specific Flexural Modulus1643 MPa/(g/cc)Flexural Modulus per density unit
Specific Flexural Strength69.47 MPa/(g/cc)Flexural Strength per density unit
Specific Tensile Modulus1925 MPa/(g/cc)Tensile Modulus per density unit
Specific Tensile Strength48.27 MPa/(g/cc)UTS per density unit
Surface Finish0.42 Ra µmAfter CNC machining
 1.83 Ra µmAfter Manual Finishing
 8.17 Ra µmAfter SLS Process

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCRPT40x / 318860

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.