MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC NORYL™ Resin N190 Polyphenylene Ether + PS (PPE+PS) (Europe)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Unreinforced

Material Notes: NORYL™ N190 resin is a non-reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This injection moldable grade contains non-brominated, non-chlorinated flame retardant and carries a UL94 flame rating of 5VA at 3mm and V0 at 1.5mm along with UL746C Outdoor Suitability rating of F1. NORYL N190 resin exhibits high impact strength, dimensional stability, hydrolytic stability, and very low moisture absorption. This material is an excellent candidate for a variety of applications such as solar frames, unattended power supply (UPS) inverter/charger, indoor and outdoor electrical enclosures / housings / connectors, and wall plates / sockets / switches. *This grade is also referred to as NORYL N1900 in several regions.

Features: Hydrolytic Stability,Flame Retardant,Non-Chlorinated,Non-Brominated,Low Warpage

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.10 g/ccISO 1183
Moisture Absorption 0.0600 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.32 %ISO 62-1
Viscosity 8.0 cP
@Load 2.16 kg,
Temperature 280 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cmSABIC method
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 87.0 MPaH358/30; ISO 2039-1
Tensile Strength at Break 40.0 MPa50 mm/min; ISO 527
Tensile Strength, Yield 50.0 MPa50 mm/min; ISO 527
Elongation at Break 20 %50 mm/min; ISO 527
Elongation at Yield 3.0 %50 mm/min; ISO 527
Tensile Modulus 2300 MPa1 mm/min; ISO 527
Flexural Strength 75.0 MPayield, 2 mm/min; ISO 178
Flexural Modulus 2200 MPa2 mm/min; ISO 178
Izod Impact, Notched (ISO) 10.0 kJ/m²80*10*4; ISO 180/1A
 6.00 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Charpy Impact, Notched 10.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 5.00 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohmROA; IEC 60093
Dielectric Constant 2.6
@Frequency 1e+6 Hz
IEC 60250
 2.7
@Frequency 50.0 - 60.0 Hz
IEC 60250
Dissipation Factor 0.00040
@Frequency 50.0 - 60.0 Hz
IEC 60250
 0.00090
@Frequency 1e+6 Hz
IEC 60250
Arc Resistance 60 - 120 secASTM D495
Comparative Tracking Index 250 VIEC 60112
 400 - 600 VUL 746A
Hot Wire Ignition, HWI 60 - 120 sec
@Thickness >=1.50 mm
UL 746A
High Amp Arc Ignition, HAI 60 - 120 arcs
@Thickness >=1.50 mm
UL 746A
High Voltage Arc-Tracking Rate, HVTR >= 150 mm/minUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 70.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 90.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
Thermal Conductivity 0.250 W/m-KISO 8302
Hot Ball Pressure Test 75.0 °CPASS; IEC 60695-10-2
 95.0 °CIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °CEdgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °CEdgew 120*10*4 sp=100mm; ISO 75/Ae
Vicat Softening Point 95.0 °CRate B/50; ISO 306
 105 °CRate B/120; ISO 306
 110 °CRate A/50; ISO 306
UL RTI, Electrical 95.0 °CUL 746B
UL RTI, Mechanical with Impact 80.0 °CUL 746B
UL RTI, Mechanical without Impact 95.0 °CUL 746B
Flammability, UL94 V-0
@Thickness >=1.50 mm
UL 94
 5VA
@Thickness >=3.00 mm
UL 94
Oxygen Index 30 %ISO 4589
Glow Wire Flammability Index 960 °C
@Thickness 3.20 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 240 - 260 °C
Zone 2 240 - 260 °C
Zone 3 260 - 280 °C
Melt Temperature 260 - 280 °CInjection Molding
Mold Temperature 60.0 - 80.0 °C
Drying Temperature 80.0 - 100 °CInjection Molding
Dry Time 2.00 - 3.00 hourInjection Molding
Precipitation Temperature 60.0 - 80.0 °CHopper Temperature
 
Descriptive Properties
UV-light, water exposure/immersionF1UL 746C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82361 / 290308

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.