MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC NORYL™ Resin NHP9023 Polyphenylene Ether + PS (PPE+PS) (Europe)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Unreinforced

Material Notes: NORYL™ NHP9023 resin is a 15% glass reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This injection moldable grade contains non-brominated, non-chlorinated flame retardant and carries a UL94 flame rating of V0 1.5mm and V1 at 0.75mm for thin-wall molding capability. NORYL NHP9023 is based on a unique co-polymer technology and exhibits good dimensional stability, high heat resistance, strong electrical performance, and very low specific gravity. It is an excellent candidate for copier fuser units, business equipment internal components, and electrical applications where thin-wall FR, modulus retention, and high heat resistance are required.

Features: Hydrolytic Stability,Low Creep Sensitivity,High Heat Resistance,Good Stiffness,Non-Halogenated,Non-Chlorinated,Non-Brominated,Low Warpage,Good Processability,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.21 g/cc1.21 g/ccASTM D792
Density 1.21 g/cc0.0437 lb/in³ISO 1183
Moisture Absorption 0.0200 %0.0200 %Injection Molding
 0.110 %0.110 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.20 %0.20 %ISO 62-1
Viscosity 17 cP
@Load 10.0 kg,
Temperature 280 °C
17 cP
@Load 22.0 lb,
Temperature 536 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0038 cm/cm0.0038 in/inSABIC method
Melt Flow 20 g/10 min
@Load 5.00 kg,
Temperature 300 °C
20 g/10 min
@Load 11.0 lb,
Temperature 572 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 121121ASTM D785
Tensile Strength at Break 90.0 MPa13100 psi5 mm/min; ISO 527
 112 MPa16200 psi5 mm/min; ASTM D638
Elongation at Break 2.7 %2.7 %5 mm/min; ISO 527
 2.9 %2.9 %5 mm/min; ASTM D638
Tensile Modulus 5.40 GPa783 ksi5 mm/min; ASTM D638
 5.50 GPa798 ksi1 mm/min; ISO 527
Flexural Strength 140 MPa20300 psiyield, 2 mm/min; ISO 178
 163 MPa23600 psiyld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 4.90 GPa711 ksi2 mm/min; ISO 178
 5.20 GPa754 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 500 J369 ft-lbASTM D256
Izod Impact, Notched (ISO) 7.00 kJ/m²3.33 ft-lb/in²80*10*4; ISO 180/1A
 6.00 kJ/m²
@Temperature -30.0 °C
2.86 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 27.0 kJ/m²12.8 ft-lb/in²80*10*4; ISO 180/1U
 28.0 kJ/m²
@Temperature -30.0 °C
13.3 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1U
Charpy Impact Unnotched 2.70 J/cm²12.8 ft-lb/in²Edgew 80*10*3 sp=62mm; ISO 179/1eU
 3.10 J/cm²
@Temperature -30.0 °C
14.8 ft-lb/in²
@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 0.700 J/cm²3.33 ft-lb/in²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 175 V175 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  35.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
19.4 µin/in-°F
@Temperature 73.4 - 176 °F
ISO 11359-2
 38.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
21.1 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow 64.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
35.6 µin/in-°F
@Temperature 73.4 - 176 °F
ISO 11359-2
Hot Ball Pressure Test 125 °C257 °FPASS; IEC 60695-10-2
Deflection Temperature at 1.8 MPa (264 psi) 153 °C
@Thickness 6.40 mm
307 °F
@Thickness 0.252 in
unannealed; ASTM D648
Vicat Softening Point 161 °C322 °FRate B/50; ISO 306
 163 °C325 °FRate B/120; ISO 306
Glow Wire Flammability Index 960 °C
@Thickness 3.20 mm
1760 °F
@Thickness 0.126 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 300 - 325 °C572 - 617 °F
Zone 2 275 - 320 °C527 - 608 °F
Zone 3 290 - 325 °C554 - 617 °F
Melt Temperature 300 - 325 °C572 - 617 °FInjection Molding
Mold Temperature 80.0 - 110 °C176 - 230 °F
Drying Temperature 110 - 120 °C230 - 248 °FInjection Molding
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hourInjection Molding
 8.00 hour8.00 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Shot Size 30 - 70 %30 - 70 %
Screw Speed 20 - 100 rpm20 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH82409 / 290356

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.