MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) TegraCore™ R-1050 PPSU Polyphenylsulfone Foam
Categories: Other Engineering Material; Composite Core Material; Polymer; Thermoplastic; Polyphenylsulfone (PPSU)

Material Notes: Tegracore™ R-1050 is a high-performance foam based on Radel® polyphenylsulfone, a versatile, super-tough thermoplastic with a long history of success in structural and decorative aircraft interior components. Tegracore™ R-1050 foam exhibits exceptionally high damage tolerance and withstands prolonged exposure to water, aggressive chemicals including Skydrol® and jet fuel, and temperatures ranging from -40°C to 204°C (-40°F to 400°F).

In addition, it is compliant with aerospace flame/smoke and toxicity (FST) standards. R-1050 foam can be continuously produced in shapes, making it particularly well-suited to implement cost-effective, highly automated interior part production processes. Because R-1050 foam is fully thermoplastic, it can be repaired and recycled. It can be cut, bonded and formed with conventional equipment.

Coefficient of Linear Thermal Expansion - ASTM E831 (-65 to 175°C): 42 cm/cm/°C; Coefficient of Linear Thermal Expansion - ASTM E831 (-65 to 175°C): 44 cm/cm/°C; Coefficient of Linear Thermal Expansion - GE (-65 to 175°C): 55 cm/cm/°C; NBS Smoke Density - FAR 25.853 2.00; NBS Smoke Density - F814/E662 2.00; OSU Test - FAR 25.853 35.0 kW·min/m²; OSU Test - FAR 25.853 < 30.0 kW·min/m²; R-Value - (2.54 cm): 0.64 m²·K/W; Toxicity - BSS 7239/ATS 1000/ABD 0031 < 1 ppm; Toxicity - BSS 7239/ATS 1000/ABD 0031 < 2 ppm; Toxicity - BSS 7239/ATS 1000/ABD 0031 < 1 ppm; Toxicity - BSS 7239/ATS 1000/ABD 0031 < 1 ppm; Toxicity - BSS 7239/ATS 1000/ABD 0031 < 1 ppm; Vertical Burn - 60 second - DMS 1510 60.0 mm; Vertical Burn - 60 second - FAR 25.853 4.0 sec; Vertical Burn - 60 second - DMS 1510 0.0 sec

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.0500 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 1.90 MPaASTM D638
Compressive Strength 0.620 MPaASTM D695
Compressive Modulus 23.0 MPaASTM D695
Shear Modulus 0.00930 GPaASTM D732
Shear Strength 0.690 MPaASTM D732
 
Thermal PropertiesOriginal ValueComments
CTE, linear 42.0 µm/m-°C
@Temperature -65.0 - 175 °C
ASTM E831
Thermal Conductivity 0.0380 W/m-K
@Temperature 20.0 °C
ASTM C177
 0.0390 W/m-K
@Temperature 200 °C
ASTM C177
Maximum Service Temperature, Air 400 °F
Minimum Service Temperature, Air -40.0 °C
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 North America
ProcessingFoam Processing

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4541 / 280341

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.