MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hexcel® HexPly® 250CB Phenolic Resin
Categories: Polymer; Thermoset; Phenolic

Material Notes: Description: HexPly®250CB is as 250C with an improved surface finish. HexPly® 200 is a phenolic resin used extensively in fire proof components such as engine cowlings, fire walls, rocket nozzles and exit gas cones. The low smoke density and very low toxicity during ignition meet the requirements of FAR 25 and ATS 1000-001 specifications. The HexPly® 200 system has excellent ablative resistance and is available in fabric reinforcements and single tows.

Benefits and Features

  • Qualified for aerospace and ground transport Fire, Smoke and Toxicity (FST) specifications
  • Controlled flow matrix
  • Excellent tack life
  • Self extinguishing
  • Good peel properties

Information provided by Hexcel Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.15 g/cc0.0415 lb/in³
 
Processing PropertiesMetricEnglishComments
Cure Time  30.0 min
@Temperature 150 °C
0.500 hour
@Temperature 302 °F
 90.0 min
@Temperature 135 °C
1.50 hour
@Temperature 275 °F
Gel Time  7.00 min
@Temperature 160 °C
7.00 min
@Temperature 320 °F
 16.0 min
@Temperature 135 °C
16.0 min
@Temperature 275 °F
 72.0 min
@Temperature 105 °C
72.0 min
@Temperature 221 °F
Shelf Life 12.0 Month
@Temperature -18.0 °C
12.0 Month
@Temperature -0.400 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHEXCB9186 / 322342

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.