MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger TECAPEI™ shapes combine Ultem® PEI polymer with Ensinger's proprietary extrusion techniques for exceptional reliability, consistency, dimensional stability, and high temperature mechanical performance. FDA, USP Class VI and NSF compliant.

SABIC ULTEM™ Resin HU2100 Polyetherimide (PEI) (Americas)
Categories: Polymer; Thermoplastic; Polyetherimide (PEI)

Material Notes: 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). US FDA and European Food Contact approved. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI); food contact compliant; Steam, Gamma, EtO, and E-beam sterilizable.

Features: Healthcare,High Stiffness,Steam, Gamma, EtO and E-beam sterilizable,Hydrolytic Stability,Chemical Resistance,Low Smoke and Toxicity,Good Mechanicals in Broad Temperature Range,Low Creep Sensitivity,Low Shrinkage,Good metal adhesion,Amorphous,High Strength,High Heat Resistance,Good dimensional stability,Flame Retardant,Steam Sterilizable,Gamma Sterilizable,E-beam Sterilizable,Food Contact Acceptable,Biocompatible

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.34 g/cc1.34 g/ccASTM D792
Density 1.34 g/cc0.0484 lb/in³ISO 1183
Moisture Absorption 0.0200 %0.0200 %Injection Molding
 0.600 %0.600 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 1.0 %1.0 %ISO 62-1
Viscosity 9.0 cP
@Load 5.00 kg,
Temperature 360 °C
9.0 cP
@Load 11.0 lb,
Temperature 680 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0050 - 0.0060 cm/cm
@Thickness 3.20 mm
0.0050 - 0.0060 in/in
@Thickness 0.126 in
SABIC method
Melt Flow 5.0 g/10 min
@Load 3.80 kg,
Temperature 200 °C
5.0 g/10 min
@Load 8.38 lb,
Temperature 392 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 115 MPa16700 psi5 mm/min; ASTM D638
 115 MPa16700 psi5 mm/min; ISO 527
Tensile Strength, Yield 114 MPa16500 psi5 mm/min; ASTM D638
 115 MPa16700 psi5 mm/min; ISO 527
Elongation at Break 4.0 %4.0 %5 mm/min; ISO 527
 6.0 %6.0 %5 mm/min; ASTM D638
Elongation at Yield 4.0 %4.0 %5 mm/min; ISO 527
 6.0 %6.0 %5 mm/min; ASTM D638
Tensile Modulus 4.50 GPa653 ksi1 mm/min; ISO 527
 4.68 GPa679 ksi5 mm/min; ASTM D638
Flexural Strength 160 MPa23200 psiyld, 1.3 mm/min, 50 mm span; ASTM D790
 185 MPa26800 psibreak, 2mm/min; ISO 178
Flexural Modulus 4.50 GPa653 ksi2 mm/min; ISO 178
 5.50 GPa798 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 53.0 J39.1 ft-lbASTM D256
 53.0 J
@Temperature -30.0 °C
39.1 ft-lb
@Temperature -22.0 °F
ASTM D256
Izod Impact, Unnotched (ISO) 30.0 kJ/m²14.3 ft-lb/in²80*10*4; ISO 180/1U
 30.0 kJ/m²
@Temperature -30.0 °C
14.3 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1U
Charpy Impact, Notched 0.700 J/cm²3.33 ft-lb/in²Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 10.0 J7.38 ft-lbASTM D3763
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 15.0 kV/mm
@Thickness 3.20 mm
381 kV/in
@Thickness 0.126 in
in oil; IEC 60243-1
Arc Resistance 60 - 120 sec60 - 120 secASTM D495
Comparative Tracking Index 100 - 175 V100 - 175 VUL 746A
 150 V150 VIEC 60112
Hot Wire Ignition, HWI  30 - 60 sec
@Thickness >=1.50 mm
30 - 60 sec
@Thickness >=0.0591 in
UL 746A
 60 - 120 sec
@Thickness >=3.00 mm
60 - 120 sec
@Thickness >=0.118 in
UL 746A
High Amp Arc Ignition, HAI  0.00 - 15 arcs
@Thickness >=3.00 mm
0.00 - 15 arcs
@Thickness >=0.118 in
UL 746A
 15 - 30 arcs
@Thickness >=1.50 mm
15 - 30 arcs
@Thickness >=0.0591 in
UL 746A
High Voltage Arc-Tracking Rate, HVTR 25.4 - 80.0 mm/min1.00 - 3.15 in/minUL 746A
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  26.0 µm/m-°C
@Temperature 23.0 - 150 °C
14.4 µin/in-°F
@Temperature 73.4 - 302 °F
ISO 11359-2
 32.4 µm/m-°C
@Temperature -40.0 - 40.0 °C
18.0 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
CTE, linear, Transverse to Flow  60.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
33.3 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 60.0 µm/m-°C
@Temperature 23.0 - 150 °C
33.3 µin/in-°F
@Temperature 73.4 - 302 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 205 °C401 °FEdgew 120*10*4 sp=100mm; ISO 75/Ae
 205 °C
@Thickness 3.20 mm
401 °F
@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 212 °C414 °FRate B/50; ISO 306
 217 °C423 °FRate B/120; ISO 306
 223 °C433 °FRate B/50; ASTM D1525
UL RTI, Electrical 170 °C338 °FUL 746B
UL RTI, Mechanical with Impact 170 °C338 °FUL 746B
UL RTI, Mechanical without Impact 170 °C338 °FUL 746B
Flammability, UL94  V-0
@Thickness >=0.410 mm
V-0
@Thickness >=0.0161 in
UL 94
 5VA
@Thickness >=1.90 mm
5VA
@Thickness >=0.0748 in
UL 94
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 350 - 405 °C662 - 761 °F
Zone 2 350 - 405 °C662 - 761 °F
Zone 3 360 - 415 °C680 - 779 °F
Melt Temperature 370 - 410 °C698 - 770 °FInjection Molding
Mold Temperature 140 - 180 °C284 - 356 °F
Drying Temperature 150 °C302 °FInjection Molding
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hourInjection Molding
Precipitation Temperature 80.0 - 120 °C176 - 248 °FHopper Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH82722 / 290669

Ensinger SPI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.